40% Glass Fiber Reinforced LCP is a subcategory of Liquid Crystal Polymer. The additative is added by weight during the manufacturing process.
Liquid Crystal Polymer, also known as LCP, is a thermoplastic. Common trade names are Vectra and Xydar. Although expensive, LCP has excellent strength and good high temperature properties. It can be used in thin wall (as thin as 0.2 mm) applications. LCP parts can withstand vapor phase reflow and autoclaving temperatures of 135 ºC. It has high chemical resistance and is flame retardant. It has very low coefficient of thermal expansion and high tensile modulus (from 10 to 24 GPa). LCP is commonly used in high-performance engineering applications such as electrical connectors and machine parts. It can be used in surgical devices, and some LCP's meet the standards of USP Class VI.
Additional Information
Other common Liquid Crystal Polymer (LCP) include 45% Glass Fiber Reinforced HDT LCP, 30% Mineral Filled LCP, Glass Fiber Reinforced Used for SMT LCP, Unfilled Medium Melting Point LCP, 30% Carbon Fiber Reinforced LCP, 50% Mineral Filled LCP, 30% Glass Fiber Reinforced LCP, 30% Glass Fiber Reinforced High HDT LCP, Unfilled Platable Grade LCP, PTFE Filled LCP, 15% Glass Fiber Reinforced LCP, and Glass / Mineral Filled LCP.
Related Glossary Pages
Glossary: Materials: Polymers: Polyester: Poly(cyclohexylene-Methylene-Terephthalate): 40% Glass: Flame-Retardant
Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C93400 Glossary: Materials: Alloys: Copper Alloy: Wire: AWG-35 Glossary: Materials: Polymers: Polyamide: Nylon (PA 66): 10% PTFE: Lubricated Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A284 Grade D Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1045 Glossary: Materials: Polymers: Polyacrylates: Poly(methylmethacrylate), PMMA: Molding and Extrusion Compounds Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C19500 Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1035 Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 316F Related Pages
eFunda Polymers: Properties of Liquid Crystal Polymer {unfilled ...
eFunda Polymers: Properties of Liquid Crystal Polymer {unfilled, platable grade}
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 40 ...
... of Polyamide {nylon (PA 6), 40% mineral and glass fiber reinforced} ... State: nylon (PA 6). Additives: 40% mineral and glass fiber reinforced ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 25% glass ...
State: nylon (PA 6). Additives: 25% glass fiber reinforced ... Coef of Thermal Expansion (10-6/ºC), 40, D696. Deflection Temperature (ºC), 220 · 0.46 MPa ...
eFunda Polymers: Properties of Liquid Crystal Polymer {30% mineral ...
eFunda Polymers: Properties of Liquid Crystal Polymer {30% mineral filled}
eFunda: Polymer (Plastic) Supplier Contact Information
Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219. Phone: 718-851-8111
eFunda: Glossary: Units: Volume: Quart (US, Liquid)
eFunda Polymers: Listing of Liquid Crystal Polymer (Vectra, Xydar). Liquid Crystal Polymer, also known as LCP, has been mass-produced since 1980. ...
eFunda Polymers: Properties of Polyamide {partially aromatic, 40 ...
Reinforced Plastics · Packaging Digest · Managing Automation ... State: partially aromatic. Additives: 40% glass fiber reinforced ...
eFunda Polymers: Properties of Liquid Crystal Polymer {40% glass ...
eFunda Polymers: Properties of Liquid Crystal Polymer {40% glass fiber reinforced} ... Solvay Advanced Polymers, L.L.C., Alpharetta, GA, 800-621-4557 ...
eFunda: Listing of Common Polymers (Plastics) in Chronological Order
Applications include surgical devices, and some LCP's meet the standards of USP Class VI. -, It has excellent strength yet is expensive. ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 40% long ...
Reinforced Plastics · Packaging Digest · Evaluation Engineering · appliance DESIGN ... State: nylon (PA 6). Additives: 40% long glass fiber reinforced ...
|
||||||||