Chemically Lubricated Acetal is a subcategory of Polyacetal. The additative is added during the manufacturing process.
Polyacetal, also known as Acetal, is a thermoplastic. Common trade names are Delrin and Ultraform. homopolymer It is a lubricious, strong, and resistant to creep and fatigue. It has good dimensional stability and relatively high abrasion and chemical resistance. Acetal is commonly used in quality toy parts, handles, knobs, and bearing parts. Delrin is approved by FDA for use in the food industry. Acetal resins were commonly used in the plumbing industry. However, they are sensitive to chlorine which leads to cracks in acetal plumbing fittings. The widespread failure of acetal moldings in potable and hot water supplies resulted in one of the largest class actions in the USA when acetal plumbing fittings cracked and caused floods of many homes in many states.
Additional Information
Other common Polyacetal (Acetal) include Acetal, Acetal, Impact Modified Acetal, Impact Modified Acetal, Mineral Filled Acetal, Extrusion and Blow Molding Grade Acetal, 2% Silicone Low Wear Acetal, UV Stabilized Acetal, 20% Glass Reinforced Acetal, 25% Glass Coupled Acetal, 40% Long Glass Fiber Reinforced Acetal, 21% PTFE Filled Acetal, 2 - 20% PTFE Filled Acetal, 1.5% PTFE Filled Acetal, UV Stabilized Acetal, UV Stabilized, 20% Glass Filled Acetal, Extrusion Grade Acetal, 30% Carbon Fiber EMI Shielding (conductive) Acetal, and 10% PAN Carbon Fiber, 10% PTFE Filled EMI Shielding (conductive) Acetal.
Related Glossary Pages
Glossary: Materials: Alloys: Copper Alloy: Wire: AWG-2
Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 317 Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1043 Glossary: Materials: Alloys: Magnesium Alloy: ASTM AZ31C-F Glossary: Materials: Polymers: Polyamide: Partially Aromatic: 50% Glass Fiber Reinforced Glossary: Materials: Alloys: Aluminum Alloy: Cast: A360.0 Glossary: Materials: Polymers: Polyamide: Nylon (PA 6), Semi-Aromatic Semicrystalline Copolymer: 35% Glass Fiber Reinforced Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 9310 Glossary: Materials: Polymers: Polyphenylene Sulfide: 40% Long Glass Fiber Reinforced Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C14310 Related Pages
eFunda Polymers: Properties of Acetal {homopolymer, 20% glass ...
eFunda Polymers: Properties of Acetal {homopolymer, 20% glass reinforced}
Fluid Film Bearings
Chemical Processing. What Is ISO 14001. NASA Tech Briefs. appliance DESIGN ... Various ways have been devised for keeping a journal bearing lubricated. ...
eFunda: Polymer (Plastic) Home Page
Glass Transition Temperature · Heat Deflection Temperature · Mold Shrinkage · more... Thermoplastics · ABS · Fluoropolymers · Polyacetal ...
eFunda Polymers: Properties of Acetal {homopolymer}
eFunda Polymers: Properties of Acetal {homopolymer}
eFunda: Polymer (Plastic) Supplier Contact Information
American Polymers, Inc. 53 Millbrook St. P.O. Box 60398. Worcester, MA 01606 ... Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219 ...
eFunda: Listing of Common Polymers (Plastics) in Chronological Order
Polyacetal (Acetal); 1958. -, Thermoplastic. -, Used in quality toy parts, handles and knobs, and bearing parts. -, It is lubricious, strong, ...
eFunda Polymers: Properties of Acetal {homopolymer, chemically ...
eFunda Polymers: Properties of Acetal {homopolymer, chemically lubricated}
eFunda Polymers: Listing of Liquid Crystal Polymer (Vectra, Xydar)
Liquid Crystal Polymer, also known as LCP, has been mass-produced since 1980. ... Liquid Crystal Polymer, glass fiber reinforced, used for SMT. ...
eFunda: Polymer (Plastic) Supplier Contact Information
Acetal, homopolymer, chemically lubricated. DuPont Co., Polymers. 1007 Market St
eFunda Polymers: Properties of Acetal {copolymer, 25% glass coupled}
eFunda Polymers: Properties of Acetal {copolymer, 25% glass coupled}
|
||||||||