Polyamide: Nylon (PA 6): 25% Glass Fiber Reinforced
Home |
Directory |
Career |
News |
Industrial
|
|
|
|
Glossary » Materials » Polymers » Polyamide » 25% Glass Fiber Reinforced
25% Glass Fiber Reinforced PA is a subcategory of Polyamide. The additative is added by weight during the manufacturing process.
Polyamide, also known as PA, is a thermoplastic polycondensate. Common trade names are Ultramid and Zytel. nylon (PA 6) It has high lubricity and moderate strength. It is tough, inexpensive, but has poor dimensional stability due to water absorption (hygroscopic nature). PA is commonly used to make high-lubricity parts such as bearings, blow moldings molds, and clothing fabrics.
Additional Information
Other common Polyamide (PA) include Ceramic and Glass Fiber Reinforced PA, Molding and Extrusion Compound PA, 15% Glass Fiber Reinforced PA, 30-35% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 35% Glass Fiber Reinforced PA, 45% Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Mineral and Glass Fiber Reinforced PA, 40% Mineral Reinforced PA, High Impact Copolymers and Rubber Modified Compounds PA, Unfilled With Molybdenum Disulfide PA, 30% Glass Fiber Reinforced, Impact Modified PA, 30% PAN Carbon Fiber EMI Shielding (conductive) PA, PA, Heat Stabilized PA, Oil Filled PA, Plasticized PA, Type 6 / 612 Blend PA, Molding Compound PA, 13% Glass Fiber Reinforced, Heat-Stablized PA, 15% Glass Fiber Reinforced PA, 30-33% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 60% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 15-33% Glass Fiber Reinforced, Toughened PA, 25-30% Mineral Filled, Modified High-Impact PA, Unreinforced Flame-Retardant Grade PA, 20-25% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Glass and Mineral Reinforced PA, 40-45% Mineral Filled PA, 30% Graphite Or PAN Carbon Fiber PA, 40% Aluminum Flake EMI Shielding (conductive) PA, 5% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 6% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 10% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 50% PAN Carbon Fiber EMI Shielding (conductive) PA, 30% Pitch Carbon Fiber EMI Shielding (conductive) PA, 40% Pitch Carbon Fiber EMI Shielding (conductive) PA, 15% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, 40% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, Molybdenum Disulfide Filled Antifriction PA, 5% Silicone Lubricated PA, 10% PTFE Lubricated PA, 30% PTFE Lubricated PA, 5% Molydenum Disulfide and 30% PTFE Lubricated PA, PA, Molding and Extrusion Compound PA, 30-40% Long Glass Fiber Reinforced PA, 30-40% Long Glass Fiber Reinforced PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, Molding Compound PA, 30-35% Glass Fiber Reinforced PA, 35-45% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flamed-Retardant Grade PA, 10% PTFE Lubricated PA, 15% PTFE, 30% Glass Fiber Reinforced Lubricated PA, 10% PTFE, 30% PAN Carbon Fiber Lubricated PA, Extrusion PA, Unreinforced PA, Super-Tough PA, 15% Glass Reinforced PA, 15% Glass Reinforced V-O PA, 30% Glass Reinforced PA, 30% Glass Reinforced V-O PA, 50% Glass Reinforced PA, 50% Glass and Mineral Filled PA, Molding and Extrusion Compound PA, Molding and Extrusion Compound PA, PA, Unfilled Aramid Molded Parts PA, 35% Glass Fiber Reinforced, Impact Modified PA, 40% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, and 60% Glass Fiber Reinforced PA.
Related Glossary Pages
Glossary: Materials: Alloys: Magnesium Alloy: ASTM AZ91B-F
Glossary: Materials: Alloys: Titanium Alloy: Wrought: Ti-5Al-2.5Sn-ELI (low O2) Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A414 Grade E Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C97400 Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C43400 Glossary: Units: Pressure: Micron of Mercury (millitorr) Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C37000 Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A514 Type N Glossary: Materials: Alloys: Titanium Alloy: Wrought: Ti-6Al-2Sn-4Zr-6Mo Glossary: Materials: Polymers: Polyamide: Nylon (PA 66): 60% Long Glass Fiber Reinforced Related Pages
eFunda: Listing of Common Polymers (Plastics)
eFunda: Listing of Common Polymers (Plastics) ... Cellulosic, Thermoplastic modified natural polymer substance. Epoxy, Thermoset polyadduct. ...
eFunda Polymers: Properties of Fluoroplastics {modified PE-TFE, 25 ...
... Polymers: Properties of Fluoroplastics {modified PE-TFE, 25% glass fiber reinforced} ... State: modified PE-TFE. Additives: 25% glass fiber reinforced ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 25% glass ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 25% glass fiber reinforced} ... State: nylon (PA 6). Additives: 25% glass fiber reinforced ...
eFunda: Glossary of Polymers (Plastics)
Common terms used in material science of polymers.
eFunda: Polymer (Plastic) Supplier Contact Information
Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219. Phone: 718-851-8111
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 30-33 ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 30-33% glass fiber reinforced}
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast, plasticized}
eFunda Polymers: Properties of Polyamide {nylon (PA 66), molding ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), molding compound}
eFunda Polymers: Listing of Polyester (Valox, Celanex)
Polyester (thermoplastic), poly(butylene-terephthalate), 60% long glass fiber reinforced. 10. Polyester (thermoplastic), poly(butylene-terephthalate), 25% ...
eFunda: Listing of Common Polymers (Plastics) in Chronological Order
It is tough, inexpensive, and has poor dimensional stability due to water absorption (hygroscopic nature). -, Trade Name: Ultramid, Zytel. ...
|
||||||||