Polyamide: Nylon (PA 6): 30% Long Glass Fiber Reinforced
Home |
Directory |
Career |
News |
Industrial
|
|
|
|
Glossary » Materials » Polymers » Polyamide » 30% Long Glass Fiber Reinforced
30% Long Glass Fiber Reinforced PA is a subcategory of Polyamide. The additative is added by weight during the manufacturing process. Its tensile strength ranges from 25200 to 26000 MPa at break. Its flexural strength ranges from 38800 to 40000 MPa. Its compressive strength ranges from 24000 to 32200 MPa. Its elongation at break ranges from 2.3 to 2.5 %. Its hardness ranges from 93 to 96 Rockwell M. Its melting temperature ranges from 210 to 220 °C. Its molding pressure ranges from 10 to 20 MPa.
Polyamide, also known as PA, is a thermoplastic polycondensate. Common trade names are Ultramid and Zytel. nylon (PA 6) It has high lubricity and moderate strength. It is tough, inexpensive, but has poor dimensional stability due to water absorption (hygroscopic nature). PA is commonly used to make high-lubricity parts such as bearings, blow moldings molds, and clothing fabrics.
Additional Information
Other common Polyamide (PA) include Ceramic and Glass Fiber Reinforced PA, Molding and Extrusion Compound PA, 15% Glass Fiber Reinforced PA, 25% Glass Fiber Reinforced PA, 30-35% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 35% Glass Fiber Reinforced PA, 45% Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Mineral and Glass Fiber Reinforced PA, 40% Mineral Reinforced PA, High Impact Copolymers and Rubber Modified Compounds PA, Unfilled With Molybdenum Disulfide PA, 30% Glass Fiber Reinforced, Impact Modified PA, 30% PAN Carbon Fiber EMI Shielding (conductive) PA, PA, Heat Stabilized PA, Oil Filled PA, Plasticized PA, Type 6 / 612 Blend PA, Molding Compound PA, 13% Glass Fiber Reinforced, Heat-Stablized PA, 15% Glass Fiber Reinforced PA, 30-33% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 60% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 15-33% Glass Fiber Reinforced, Toughened PA, 25-30% Mineral Filled, Modified High-Impact PA, Unreinforced Flame-Retardant Grade PA, 20-25% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Glass and Mineral Reinforced PA, 40-45% Mineral Filled PA, 30% Graphite Or PAN Carbon Fiber PA, 40% Aluminum Flake EMI Shielding (conductive) PA, 5% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 6% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 10% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 50% PAN Carbon Fiber EMI Shielding (conductive) PA, 30% Pitch Carbon Fiber EMI Shielding (conductive) PA, 40% Pitch Carbon Fiber EMI Shielding (conductive) PA, 15% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, 40% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, Molybdenum Disulfide Filled Antifriction PA, 5% Silicone Lubricated PA, 10% PTFE Lubricated PA, 30% PTFE Lubricated PA, 5% Molydenum Disulfide and 30% PTFE Lubricated PA, PA, Molding and Extrusion Compound PA, 30-40% Long Glass Fiber Reinforced PA, 30-40% Long Glass Fiber Reinforced PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, Molding Compound PA, 30-35% Glass Fiber Reinforced PA, 35-45% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flamed-Retardant Grade PA, 10% PTFE Lubricated PA, 15% PTFE, 30% Glass Fiber Reinforced Lubricated PA, 10% PTFE, 30% PAN Carbon Fiber Lubricated PA, Extrusion PA, Unreinforced PA, Super-Tough PA, 15% Glass Reinforced PA, 15% Glass Reinforced V-O PA, 30% Glass Reinforced PA, 30% Glass Reinforced V-O PA, 50% Glass Reinforced PA, 50% Glass and Mineral Filled PA, Molding and Extrusion Compound PA, Molding and Extrusion Compound PA, PA, Unfilled Aramid Molded Parts PA, 35% Glass Fiber Reinforced, Impact Modified PA, 40% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, and 60% Glass Fiber Reinforced PA.
Related Glossary Pages
Glossary: Materials: Polymers: Polycarbonate: 10% Glass Fiber Reinforced
Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A588 Grade C Glossary: Materials: Polymers: Polyethylene: Ethylene / Vinyl Acetate, Low Density Copolymer Glossary: Materials: Polymers: Polyacrylonitrile: Injection Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 1330 Glossary: Design: Oring: Material: Chemraz Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 303PlusX Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 1060 Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A441 Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 6061 Related Pages
eFunda Polymers: Listing of Polyamide-imide
eFunda Polymers: Listing of Polyamide-imide. ... Polyamide-imide, unfilled, compression and injection molding compound. 2. Polyamide-imide, 30% glass fiber ...
eFunda: Glossary of Polymers (Plastics)
Common terms used in material science of polymers.
eFunda Polymers: Properties of Polycarbonate {20 - 30% long glass ...
... Polymers: Properties of Polycarbonate {20 - 30% long glass fiber reinforced, flame-retardant grade} ... Additives: 20 - 30% long glass fiber reinforced ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 30% long ...
... Polymers: Properties of Polyamide {nylon (PA 66), 30% long glass fiber reinforced} ... State: nylon (PA 66). Additives: 30% long glass fiber reinforced ...
eFunda Polymers: Properties of Polyurethane {thermoplastic, 30 ...
... Properties of Polyurethane {thermoplastic, 30% long glass fiber reinforced} ... State: thermoplastic. Additives: 30% long glass fiber reinforced ...
eFunda Polymers: Properties of Polypropylene {homopolymer, 20 - 30 ...
... Properties of Polypropylene {homopolymer, 20 - 30% long glass fiber reinforced} ... State: homopolymer. Additives: 20 - 30% long glass fiber reinforced ...
eFunda: Polymer (Plastic) Home Page
Index page for polymers. ... General Information. Polymer Home. Glossary. Material Science. Overview · Characteristics · Comparisons. Selection Criteria ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), molding ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), molding and extrusion compound}
eFunda Polymers: Properties of ABS {30% glass fiber reinforced ...
eFunda Polymers: Properties of ABS {30% glass fiber reinforced, injection molding grade}
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast, plasticized}
|
||||||||