Polyamide: Nylon (PA 6): 30% PAN Carbon Fiber
Home |
Directory |
Career |
News |
Industrial
|
|
![]() ![]()
|
|
Glossary » Materials » Polymers » Polyamide » Nylon (PA 6) » 30% PAN Carbon Fiber » EMI Shielding (conductive)
30% PAN Carbon Fiber EMI Shielding (conductive) PA is a subcategory of Polyamide. The additative is added by weight during the manufacturing process. Its elastic modulus ranges from 2800 to 3000 MPa. Its flexural modulus ranges from 2500 to 2700 MPa. Its tensile strength ranges from 30000 to 36000 MPa at break. Its flexural strength ranges from 46000 to 51000 MPa. Its Izod Impact strength ranges from 1.5 to 2.8 J/cm. Its elongation at break ranges from 2 to 3 %. Its melting temperature ranges from 210 to 220 °C.
Polyamide, also known as PA, is a thermoplastic polycondensate. Common trade names are Ultramid and Zytel. nylon (PA 6) It has high lubricity and moderate strength. It is tough, inexpensive, but has poor dimensional stability due to water absorption (hygroscopic nature). PA is commonly used to make high-lubricity parts such as bearings, blow moldings molds, and clothing fabrics.
Additional Information
Other common Polyamide (PA) include Ceramic and Glass Fiber Reinforced PA, Molding and Extrusion Compound PA, 15% Glass Fiber Reinforced PA, 25% Glass Fiber Reinforced PA, 30-35% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 35% Glass Fiber Reinforced PA, 45% Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Mineral and Glass Fiber Reinforced PA, 40% Mineral Reinforced PA, High Impact Copolymers and Rubber Modified Compounds PA, Unfilled With Molybdenum Disulfide PA, 30% Glass Fiber Reinforced, Impact Modified PA, PA, Heat Stabilized PA, Oil Filled PA, Plasticized PA, Type 6 / 612 Blend PA, Molding Compound PA, 13% Glass Fiber Reinforced, Heat-Stablized PA, 15% Glass Fiber Reinforced PA, 30-33% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 60% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 15-33% Glass Fiber Reinforced, Toughened PA, 25-30% Mineral Filled, Modified High-Impact PA, Unreinforced Flame-Retardant Grade PA, 20-25% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Glass and Mineral Reinforced PA, 40-45% Mineral Filled PA, 30% Graphite Or PAN Carbon Fiber PA, 40% Aluminum Flake EMI Shielding (conductive) PA, 5% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 6% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 10% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 50% PAN Carbon Fiber EMI Shielding (conductive) PA, 30% Pitch Carbon Fiber EMI Shielding (conductive) PA, 40% Pitch Carbon Fiber EMI Shielding (conductive) PA, 15% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, 40% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, Molybdenum Disulfide Filled Antifriction PA, 5% Silicone Lubricated PA, 10% PTFE Lubricated PA, 30% PTFE Lubricated PA, 5% Molydenum Disulfide and 30% PTFE Lubricated PA, PA, Molding and Extrusion Compound PA, 30-40% Long Glass Fiber Reinforced PA, 30-40% Long Glass Fiber Reinforced PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, Molding Compound PA, 30-35% Glass Fiber Reinforced PA, 35-45% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flamed-Retardant Grade PA, 10% PTFE Lubricated PA, 15% PTFE, 30% Glass Fiber Reinforced Lubricated PA, 10% PTFE, 30% PAN Carbon Fiber Lubricated PA, Extrusion PA, Unreinforced PA, Super-Tough PA, 15% Glass Reinforced PA, 15% Glass Reinforced V-O PA, 30% Glass Reinforced PA, 30% Glass Reinforced V-O PA, 50% Glass Reinforced PA, 50% Glass and Mineral Filled PA, Molding and Extrusion Compound PA, Molding and Extrusion Compound PA, PA, Unfilled Aramid Molded Parts PA, 35% Glass Fiber Reinforced, Impact Modified PA, 40% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, and 60% Glass Fiber Reinforced PA.
Related Glossary Pages
Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 1050
Glossary: Materials: Polymers: Polyamide: Nylon (PA 610): 30-40% Long Glass Fiber Reinforced Glossary: Materials: Alloys: Steel: Alloy Steel: SAE 942X Glossary: Materials: Alloys: Steel: Tool Steel: AISI T2 Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A109 Temper 3 Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A225 Grade A Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C75700 Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 7005 Glossary: Materials: Polymers: Polycarbonate: 30% Glass Fiber Reinforced Glossary: Materials: Alloys: Steel: Tool Steel: AISI O2 Related Pages
eFunda Polymers: Properties of Polyamide {nylon (PA 66), molding ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), molding compound}
eFunda Polymers: Properties of ABS {7% stainless steel fiber, EMI ...
eFunda Polymers: Properties of ABS {7% stainless steel fiber, EMI shielding (
eFunda Polymers: Properties of ABS {10% stainless steel fiber, EMI ...
... of ABS {10% stainless steel fiber, EMI shielding (conductive)} ... Additives
eFunda Polymers: Listing of Polyamide-imide
eFunda Polymers: Listing of Polyamide-imide. ... Polyamide-imide, unfilled, compression and injection molding compound. 2. Polyamide-imide, 30% glass fiber ...
eFunda Polymers: Properties of Polyphenylene Sulfide {60 ...
... of Polyphenylene Sulfide {60% stainless steel, EMI shielding (conductive)} ... Additives: 60% stainless steel. Application: EMI shielding (conductive) ...
eFunda Polymers: Properties of Polyurethane {thermoplastic, 30 ...
... 30% PAN carbon fiber, EMI shielding (conductive)} ... State: thermoplastic. Additives: 30% PAN carbon fiber. Application: EMI shielding (conductive) ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66 ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), unreinforced, flame-
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast}
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast}
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 30 ...
... Properties of Polyamide {nylon (PA 66), 30% graphite or PAN carbon fiber} ... State: nylon (PA 66). Additives: 30% graphite or PAN carbon fiber ...
eFunda Polymers: Properties of Polyetherimide {30% carbon fiber ...
... Properties of Polyetherimide {30% carbon fiber, EMI shielding (conductive)} ... Additives: 30% carbon fiber. Application: EMI shielding (conductive) ...
|
|||||||||||||||||||||||||