Polyamide: Nylon (PA 6): 33% Glass Fiber Reinforced, Toughened
Home |
Directory |
Career |
News |
Industrial
|
|
|
|
Glossary » Materials » Polymers » Polyamide » 33% Glass Fiber Reinforced, Toughened
33% Glass Fiber Reinforced, Toughened PA is a subcategory of Polyamide. The additative is added by weight during the manufacturing process. Its melting temperature ranges from 210 to 220 °C.
Polyamide, also known as PA, is a thermoplastic polycondensate. Common trade names are Ultramid and Zytel. nylon (PA 6) It has high lubricity and moderate strength. It is tough, inexpensive, but has poor dimensional stability due to water absorption (hygroscopic nature). PA is commonly used to make high-lubricity parts such as bearings, blow moldings molds, and clothing fabrics.
Additional Information
Other common Polyamide (PA) include Ceramic and Glass Fiber Reinforced PA, Molding and Extrusion Compound PA, 15% Glass Fiber Reinforced PA, 25% Glass Fiber Reinforced PA, 30-35% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 35% Glass Fiber Reinforced PA, 45% Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Mineral and Glass Fiber Reinforced PA, 40% Mineral Reinforced PA, High Impact Copolymers and Rubber Modified Compounds PA, Unfilled With Molybdenum Disulfide PA, 30% Glass Fiber Reinforced, Impact Modified PA, 30% PAN Carbon Fiber EMI Shielding (conductive) PA, PA, Heat Stabilized PA, Oil Filled PA, Plasticized PA, Type 6 / 612 Blend PA, Molding Compound PA, 13% Glass Fiber Reinforced, Heat-Stablized PA, 15% Glass Fiber Reinforced PA, 30-33% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 60% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 15-33% Glass Fiber Reinforced, Toughened PA, 25-30% Mineral Filled, Modified High-Impact PA, Unreinforced Flame-Retardant Grade PA, 20-25% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Glass and Mineral Reinforced PA, 40-45% Mineral Filled PA, 30% Graphite Or PAN Carbon Fiber PA, 40% Aluminum Flake EMI Shielding (conductive) PA, 5% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 6% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 10% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 50% PAN Carbon Fiber EMI Shielding (conductive) PA, 30% Pitch Carbon Fiber EMI Shielding (conductive) PA, 40% Pitch Carbon Fiber EMI Shielding (conductive) PA, 15% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, 40% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, Molybdenum Disulfide Filled Antifriction PA, 5% Silicone Lubricated PA, 10% PTFE Lubricated PA, 30% PTFE Lubricated PA, 5% Molydenum Disulfide and 30% PTFE Lubricated PA, PA, Molding and Extrusion Compound PA, 30-40% Long Glass Fiber Reinforced PA, 30-40% Long Glass Fiber Reinforced PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, Molding Compound PA, 30-35% Glass Fiber Reinforced PA, 35-45% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flamed-Retardant Grade PA, 10% PTFE Lubricated PA, 15% PTFE, 30% Glass Fiber Reinforced Lubricated PA, 10% PTFE, 30% PAN Carbon Fiber Lubricated PA, Extrusion PA, Unreinforced PA, Super-Tough PA, 15% Glass Reinforced PA, 15% Glass Reinforced V-O PA, 30% Glass Reinforced PA, 30% Glass Reinforced V-O PA, 50% Glass Reinforced PA, 50% Glass and Mineral Filled PA, Molding and Extrusion Compound PA, Molding and Extrusion Compound PA, PA, Unfilled Aramid Molded Parts PA, 35% Glass Fiber Reinforced, Impact Modified PA, 40% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, and 60% Glass Fiber Reinforced PA.
Related Glossary Pages
Glossary: Materials: Polymers: Polyacetal: Homopolymer: 20% Glass Reinforced
Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C19000 Glossary: Materials: Polymers: Polyester: Poly(ethylene-Terephthalate Glycol): Unfilled PETG Glossary: Materials: Polymers: Polyethersulfone: 20% Mineral Filled Glossary: Materials: Polymers: Thermoplastic Elastomers: Polyolefin: High Hardness Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 309SCb Glossary: Materials: Polymers: Polyamide: Partially Aromatic: 50% Glass Fiber Reinforced Glossary: Materials: Alloys: Steel: Stainless Steel: 18-2FM Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 430Ti Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A441 Related Pages
eFunda: Glossary: Units: Fracture Toughness: Pa-Sqrt(meter)
eFunda Glossary for Units, Category:Fracture Toughness, Unit name: Pa-Sqrt(meter
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast, Type ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast, Type 6 / 612 blend
eFunda: Pressure Unit Category
kip/in, ksi, KSI, 6.89476x106 Pa ... mmHg, torr, Torr (0 °C), 133.322 Pa. ·, millimeter of water (15.56°C) · mmH2O, mmCE (15.56 °C), 9.79706 Pa ...
eFunda Polymers: Properties of Polyester (thermoset) {glass fiber ...
Additives: glass fiber reinforced, premix chopped glass ... Coef of Thermal Expansion (10-6/ºC), 20 - 33, D696. Deflection Temperature (ºC), 205 · 1.82 MPa ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66 ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), unreinforced, toughened
eFunda Polymers: Properties of Polyamide {nylon (PA 66), molding ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), molding compound}
eFunda: Polymer (Plastic) Supplier Contact Information
Polyamide, nylon (PA 6), unreinforced, toughened. A. Schulman. 3550 West Market St. Akron, OH 44333. Toll Free: 800-662-7203. Phone: 330-666-3751 ...
eFunda: Polymer (Plastic) Supplier Contact Information
Polyamide, nylon (PA 612), unreinforced, toughened. DSM Engineering Plastic Products, Inc. 2120 Fairmont Ave. P.O. Box 14235. Reading, PA 19612 ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66 ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), unreinforced, flame-
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast}
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast}
|
||||||||