Polyamide: Nylon (PA 6): 50% Glass Fiber Reinforced
Home |
Directory |
Career |
News |
Industrial
|
|
|
|
Glossary » Materials » Polymers » Polyamide » 50% Glass Fiber Reinforced
50% Glass Fiber Reinforced PA is a subcategory of Polyamide. The additative is added by weight during the manufacturing process.
Polyamide, also known as PA, is a thermoplastic polycondensate. Common trade names are Ultramid and Zytel. nylon (PA 6) It has high lubricity and moderate strength. It is tough, inexpensive, but has poor dimensional stability due to water absorption (hygroscopic nature). PA is commonly used to make high-lubricity parts such as bearings, blow moldings molds, and clothing fabrics.
Additional Information
Other common Polyamide (PA) include Ceramic and Glass Fiber Reinforced PA, Molding and Extrusion Compound PA, 15% Glass Fiber Reinforced PA, 25% Glass Fiber Reinforced PA, 30-35% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 35% Glass Fiber Reinforced PA, 45% Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Mineral and Glass Fiber Reinforced PA, 40% Mineral Reinforced PA, High Impact Copolymers and Rubber Modified Compounds PA, Unfilled With Molybdenum Disulfide PA, 30% Glass Fiber Reinforced, Impact Modified PA, 30% PAN Carbon Fiber EMI Shielding (conductive) PA, PA, Heat Stabilized PA, Oil Filled PA, Plasticized PA, Type 6 / 612 Blend PA, Molding Compound PA, 13% Glass Fiber Reinforced, Heat-Stablized PA, 15% Glass Fiber Reinforced PA, 30-33% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 60% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 15-33% Glass Fiber Reinforced, Toughened PA, 25-30% Mineral Filled, Modified High-Impact PA, Unreinforced Flame-Retardant Grade PA, 20-25% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Glass and Mineral Reinforced PA, 40-45% Mineral Filled PA, 30% Graphite Or PAN Carbon Fiber PA, 40% Aluminum Flake EMI Shielding (conductive) PA, 5% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 6% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 10% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 50% PAN Carbon Fiber EMI Shielding (conductive) PA, 30% Pitch Carbon Fiber EMI Shielding (conductive) PA, 40% Pitch Carbon Fiber EMI Shielding (conductive) PA, 15% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, 40% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, Molybdenum Disulfide Filled Antifriction PA, 5% Silicone Lubricated PA, 10% PTFE Lubricated PA, 30% PTFE Lubricated PA, 5% Molydenum Disulfide and 30% PTFE Lubricated PA, PA, Molding and Extrusion Compound PA, 30-40% Long Glass Fiber Reinforced PA, 30-40% Long Glass Fiber Reinforced PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, Molding Compound PA, 30-35% Glass Fiber Reinforced PA, 35-45% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flamed-Retardant Grade PA, 10% PTFE Lubricated PA, 15% PTFE, 30% Glass Fiber Reinforced Lubricated PA, 10% PTFE, 30% PAN Carbon Fiber Lubricated PA, Extrusion PA, Unreinforced PA, Super-Tough PA, 15% Glass Reinforced PA, 15% Glass Reinforced V-O PA, 30% Glass Reinforced PA, 30% Glass Reinforced V-O PA, 50% Glass Reinforced PA, 50% Glass and Mineral Filled PA, Molding and Extrusion Compound PA, Molding and Extrusion Compound PA, PA, Unfilled Aramid Molded Parts PA, 35% Glass Fiber Reinforced, Impact Modified PA, 40% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, and 60% Glass Fiber Reinforced PA.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A202 Grade A
Glossary: Units: Pressure: Gigapascal Glossary: Materials: Alloys: Steel: Tool Steel: AISI M43 Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4427 Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 94B30 Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A734 Type B Glossary: Materials: Polymers: Liquid Crystal Polymer: Glass / Mineral Filled Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C35600 Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A387 Grade 5 Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1074 Related Pages
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 15-33 ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 15-33% glass fiber reinforced, toughened}
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 30-33 ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 30-33% glass fiber reinforced}
eFunda Polymers: Listing of Polyamide (Ultramid, Zytel)
Polyamide, also known as PA, or Nylon, has been mass-produced since 1935. ... Polyamide, nylon alloys, ceramic and glass fiber reinforced. ...
eFunda Polymers: Listing of Liquid Crystal Polymer (Vectra, Xydar)
Liquid Crystal Polymer, also known as LCP, has been mass-produced since 1980. ... Liquid Crystal Polymer, glass fiber reinforced, used for SMT. ...
eFunda Polymers: Properties of Epoxy {bisphenol, glass fiber ...
State: bisphenol. Additives: glass fiber reinforced. Application: molding compounds ... Coef of Thermal Expansion (10-6/ºC), 11 - 50, D696 ...
eFunda: Pressure Unit Category
kip/in, ksi, KSI, 6.89476x106 Pa ... mmHg, torr, Torr (0 °C), 133.322 Pa. ·, millimeter of water (15.56°C) · mmH2O, mmCE (15.56 °C), 9.79706 Pa ...
eFunda Polymers: Properties of Polycarbonate {50% long glass fiber ...
eFunda Polymers: Properties of Polycarbonate {50% long glass fiber reinforced} ... Additives: 50% long glass fiber reinforced ...
eFunda: Glossary: Units: Fracture Toughness: Pa-Sqrt(meter)
eFunda Glossary for Units, Category:Fracture Toughness, Unit name: Pa-Sqrt(meter
eFunda: Overview of Polymers (Plastics)
Introduction to polymers, their molecular structures and major grouping methods.
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast, Type ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast, Type 6 / 612 blend
|
||||||||