Polyamide: Nylon (PA 6): Unfilled With Molybdenum Disulfide
Home |
Directory |
Career |
News |
Industrial
|
|
|
|
Glossary » Materials » Polymers » Polyamide » Unfilled With Molybdenum Disulfide
Unfilled With Molybdenum Disulfide PA is a subcategory of Polyamide. The additative is added during the manufacturing process. Its Izod Impact strength ranges from 0.9 to 1 J/cm. Its elongation at break ranges from 60 to 80 %. Its hardness ranges from 119 to 120 Rockwell R. Its specific gravity ranges from 1.17 to 1.18. Its molding pressure ranges from 5 to 20 MPa.
Polyamide, also known as PA, is a thermoplastic polycondensate. Common trade names are Ultramid and Zytel. nylon (PA 6) It has high lubricity and moderate strength. It is tough, inexpensive, but has poor dimensional stability due to water absorption (hygroscopic nature). PA is commonly used to make high-lubricity parts such as bearings, blow moldings molds, and clothing fabrics.
Additional Information
Other common Polyamide (PA) include Ceramic and Glass Fiber Reinforced PA, Molding and Extrusion Compound PA, 15% Glass Fiber Reinforced PA, 25% Glass Fiber Reinforced PA, 30-35% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 35% Glass Fiber Reinforced PA, 45% Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Mineral and Glass Fiber Reinforced PA, 40% Mineral Reinforced PA, High Impact Copolymers and Rubber Modified Compounds PA, 30% Glass Fiber Reinforced, Impact Modified PA, 30% PAN Carbon Fiber EMI Shielding (conductive) PA, PA, Heat Stabilized PA, Oil Filled PA, Plasticized PA, Type 6 / 612 Blend PA, Molding Compound PA, 13% Glass Fiber Reinforced, Heat-Stablized PA, 15% Glass Fiber Reinforced PA, 30-33% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 60% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 15-33% Glass Fiber Reinforced, Toughened PA, 25-30% Mineral Filled, Modified High-Impact PA, Unreinforced Flame-Retardant Grade PA, 20-25% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Glass and Mineral Reinforced PA, 40-45% Mineral Filled PA, 30% Graphite Or PAN Carbon Fiber PA, 40% Aluminum Flake EMI Shielding (conductive) PA, 5% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 6% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 10% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 50% PAN Carbon Fiber EMI Shielding (conductive) PA, 30% Pitch Carbon Fiber EMI Shielding (conductive) PA, 40% Pitch Carbon Fiber EMI Shielding (conductive) PA, 15% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, 40% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, Molybdenum Disulfide Filled Antifriction PA, 5% Silicone Lubricated PA, 10% PTFE Lubricated PA, 30% PTFE Lubricated PA, 5% Molydenum Disulfide and 30% PTFE Lubricated PA, PA, Molding and Extrusion Compound PA, 30-40% Long Glass Fiber Reinforced PA, 30-40% Long Glass Fiber Reinforced PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, Molding Compound PA, 30-35% Glass Fiber Reinforced PA, 35-45% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flamed-Retardant Grade PA, 10% PTFE Lubricated PA, 15% PTFE, 30% Glass Fiber Reinforced Lubricated PA, 10% PTFE, 30% PAN Carbon Fiber Lubricated PA, Extrusion PA, Unreinforced PA, Super-Tough PA, 15% Glass Reinforced PA, 15% Glass Reinforced V-O PA, 30% Glass Reinforced PA, 30% Glass Reinforced V-O PA, 50% Glass Reinforced PA, 50% Glass and Mineral Filled PA, Molding and Extrusion Compound PA, Molding and Extrusion Compound PA, PA, Unfilled Aramid Molded Parts PA, 35% Glass Fiber Reinforced, Impact Modified PA, 40% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, and 60% Glass Fiber Reinforced PA.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A517 Grade F
Glossary: Units: Pressure: Hectopascal Glossary: Materials: Alloys: Steel: Tool Steel: AISI T5 Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 302 Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C33200 Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C10300 Glossary: Materials: Polymers: Polysulfone: Polysulfone: 20% Glass Fiber Reinforced Glossary: Design: Oring: Material: Polyacrylate Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 422 Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A633 Grade B Related Pages
eFunda Polymers: Properties of Polyamide {nylon (PA 66 ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), unreinforced, flame-
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast, Type ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast, Type 6 / 612 blend
eFunda: Overview of Polymers (Plastics)
Introduction to polymers, their molecular structures and major grouping methods.
eFunda: Glossary of Polymers (Plastics)
Common terms used in material science of polymers.
eFunda: Polymer (Plastic) Supplier Contact Information
Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219. Phone: 718-851-8111 ... Bamberger Polymers, Inc. 2 Jericho Plaza. Jericho, NY 11753 ...
eFunda: Listing of Common Polymers (Plastics) in Chronological Order
It is tough, inexpensive, and has poor dimensional stability due to water absorption (hygroscopic nature). -, Trade Name: Ultramid, Zytel. ...
eFunda: Polymer (Plastic) Home Page
Index page for polymers. ... General Information. Polymer Home. Glossary. Material Science. Overview · Characteristics · Comparisons. Selection Criteria ...
eFunda: Pressure Unit Category
kip/in, ksi, KSI, 6.89476x106 Pa ... mmHg, torr, Torr (0 °C), 133.322 Pa. ·, millimeter of water (15.56°C) · mmH2O, mmCE (15.56 °C), 9.79706 Pa ...
eFunda Polymers: Listing of Polyamide-imide
eFunda Polymers: Listing of Polyamide-imide. ... Polyamide-imide, unfilled, compression and injection molding compound. 2. Polyamide-imide, 30% glass fiber ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast}
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast}
|
||||||||