Polyamide: Nylon (PA 610): 30-40% Long Glass Fiber Reinforced
Home |
Directory |
Career |
News |
Industrial
|
|
|
|
Glossary » Materials » Polymers » Polyamide » 30-40% Long Glass Fiber Reinforced
30-40% Long Glass Fiber Reinforced PA is a subcategory of Polyamide. The additative is added by weight during the manufacturing process. Its elastic modulus ranges from 950 to 1600 MPa. Its flexural modulus ranges from 1200 to 1430 MPa. Its tensile strength ranges from 22400 to 25400 MPa at break. Its flexural strength ranges from 34000 to 37400 MPa. Its Izod Impact strength ranges from 3.2 to 4.2 J/cm. Its elongation at break ranges from 4 to 4.1 %. Its hardness ranges from 42 to 56 Rockwell E. Its specific gravity ranges from 1.33 to 1.39.
Polyamide, also known as PA, is a thermoplastic polycondensate. Common trade names are Ultramid and Zytel. nylon (PA 610) It has high lubricity and moderate strength. It is tough, inexpensive, but has poor dimensional stability due to water absorption (hygroscopic nature). PA is commonly used to make high-lubricity parts such as bearings, blow moldings molds, and clothing fabrics.
Additional Information
Other common Polyamide (PA) include Ceramic and Glass Fiber Reinforced PA, Molding and Extrusion Compound PA, 15% Glass Fiber Reinforced PA, 25% Glass Fiber Reinforced PA, 30-35% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 35% Glass Fiber Reinforced PA, 45% Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Mineral and Glass Fiber Reinforced PA, 40% Mineral Reinforced PA, High Impact Copolymers and Rubber Modified Compounds PA, Unfilled With Molybdenum Disulfide PA, 30% Glass Fiber Reinforced, Impact Modified PA, 30% PAN Carbon Fiber EMI Shielding (conductive) PA, PA, Heat Stabilized PA, Oil Filled PA, Plasticized PA, Type 6 / 612 Blend PA, Molding Compound PA, 13% Glass Fiber Reinforced, Heat-Stablized PA, 15% Glass Fiber Reinforced PA, 30-33% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 60% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 15-33% Glass Fiber Reinforced, Toughened PA, 25-30% Mineral Filled, Modified High-Impact PA, Unreinforced Flame-Retardant Grade PA, 20-25% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Glass and Mineral Reinforced PA, 40-45% Mineral Filled PA, 30% Graphite Or PAN Carbon Fiber PA, 40% Aluminum Flake EMI Shielding (conductive) PA, 5% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 6% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 10% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 50% PAN Carbon Fiber EMI Shielding (conductive) PA, 30% Pitch Carbon Fiber EMI Shielding (conductive) PA, 40% Pitch Carbon Fiber EMI Shielding (conductive) PA, 15% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, 40% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, Molybdenum Disulfide Filled Antifriction PA, 5% Silicone Lubricated PA, 10% PTFE Lubricated PA, 30% PTFE Lubricated PA, 5% Molydenum Disulfide and 30% PTFE Lubricated PA, PA, Molding and Extrusion Compound PA, 30-40% Long Glass Fiber Reinforced PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, Molding Compound PA, 30-35% Glass Fiber Reinforced PA, 35-45% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flamed-Retardant Grade PA, 10% PTFE Lubricated PA, 15% PTFE, 30% Glass Fiber Reinforced Lubricated PA, 10% PTFE, 30% PAN Carbon Fiber Lubricated PA, Extrusion PA, Unreinforced PA, Super-Tough PA, 15% Glass Reinforced PA, 15% Glass Reinforced V-O PA, 30% Glass Reinforced PA, 30% Glass Reinforced V-O PA, 50% Glass Reinforced PA, 50% Glass and Mineral Filled PA, Molding and Extrusion Compound PA, Molding and Extrusion Compound PA, PA, Unfilled Aramid Molded Parts PA, 35% Glass Fiber Reinforced, Impact Modified PA, 40% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, and 60% Glass Fiber Reinforced PA.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 632
Glossary: Materials: Alloys: Magnesium Alloy: ASTM ZK51A-T5 Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1524H Glossary: Materials: Polymers: Polyester: Glass Fiber Reinforced, Preformed Chopped Roving Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C95200 Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 317LM Glossary: Materials: Polymers: Polyacetal: Homopolymer: Impact Modified Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C92800 Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 94B30H Glossary: Materials: Polymers: Polycarbonate: 35% Random Glass Mat Related Pages
eFunda Polymers: Properties of Polyamide {nylon (PA 66), copolymer}
eFunda Polymers: Properties of Polyamide {nylon (PA 66), copolymer}
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 15-33 ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 15-33% glass fiber reinforced, toughened}
eFunda: Pressure Unit Category
kip/in, ksi, KSI, 6.89476x106 Pa ... mmHg, torr, Torr (0 °C), 133.322 Pa. ·, millimeter of water (15.56°C) · mmH2O, mmCE (15.56 °C), 9.79706 Pa ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), molding ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), molding compound}
eFunda: Glossary: Units: Fracture Toughness: Pa-Sqrt(meter)
eFunda Glossary for Units, Category:Fracture Toughness, Unit name: Pa-Sqrt(meter
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast, Type ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast, Type 6 / 612 blend
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 30-35 ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 30-35% glass fiber reinforced}
eFunda: Polymer (Plastic) Supplier Contact Information
Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219. Phone: 718-851-8111
eFunda Polymers: Listing of Polyamide-imide
eFunda Polymers: Listing of Polyamide-imide. ... Polyamide-imide, unfilled, compression and injection molding compound. 2. Polyamide-imide, 30% glass fiber ...
eFunda Polymers: Properties of Polyamide {nylon (PA 610), 30-40 ...
... Properties of Polyamide {nylon (PA 610), 30-40% long glass fiber reinforced} ... State: nylon (PA 610). Additives: 30-40% long glass fiber reinforced ...
|
||||||||