Polyamide: Nylon (PA 612): 10% PTFE
Home |
Directory |
Career |
News |
Industrial
|
|
|
|
Glossary » Materials » Polymers » Polyamide » Nylon (PA 612) » 10% PTFE » Lubricated
10% PTFE Lubricated PA is a subcategory of Polyamide. The additative is added by weight during the manufacturing process. Its melting temperature ranges from 195 to 217 °C.
Polyamide, also known as PA, is a thermoplastic polycondensate. Common trade names are Ultramid and Zytel. nylon (PA 612) It has high lubricity and moderate strength. It is tough, inexpensive, but has poor dimensional stability due to water absorption (hygroscopic nature). PA is commonly used to make high-lubricity parts such as bearings, blow moldings molds, and clothing fabrics.
Additional Information
Other common Polyamide (PA) include Ceramic and Glass Fiber Reinforced PA, Molding and Extrusion Compound PA, 15% Glass Fiber Reinforced PA, 25% Glass Fiber Reinforced PA, 30-35% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 35% Glass Fiber Reinforced PA, 45% Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Mineral and Glass Fiber Reinforced PA, 40% Mineral Reinforced PA, High Impact Copolymers and Rubber Modified Compounds PA, Unfilled With Molybdenum Disulfide PA, 30% Glass Fiber Reinforced, Impact Modified PA, 30% PAN Carbon Fiber EMI Shielding (conductive) PA, PA, Heat Stabilized PA, Oil Filled PA, Plasticized PA, Type 6 / 612 Blend PA, Molding Compound PA, 13% Glass Fiber Reinforced, Heat-Stablized PA, 15% Glass Fiber Reinforced PA, 30-33% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 60% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 15-33% Glass Fiber Reinforced, Toughened PA, 25-30% Mineral Filled, Modified High-Impact PA, Unreinforced Flame-Retardant Grade PA, 20-25% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Glass and Mineral Reinforced PA, 40-45% Mineral Filled PA, 30% Graphite Or PAN Carbon Fiber PA, 40% Aluminum Flake EMI Shielding (conductive) PA, 5% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 6% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 10% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 50% PAN Carbon Fiber EMI Shielding (conductive) PA, 30% Pitch Carbon Fiber EMI Shielding (conductive) PA, 40% Pitch Carbon Fiber EMI Shielding (conductive) PA, 15% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, 40% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, Molybdenum Disulfide Filled Antifriction PA, 5% Silicone Lubricated PA, 10% PTFE Lubricated PA, 30% PTFE Lubricated PA, 5% Molydenum Disulfide and 30% PTFE Lubricated PA, PA, Molding and Extrusion Compound PA, 30-40% Long Glass Fiber Reinforced PA, 30-40% Long Glass Fiber Reinforced PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, Molding Compound PA, 30-35% Glass Fiber Reinforced PA, 35-45% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flamed-Retardant Grade PA, 15% PTFE, 30% Glass Fiber Reinforced Lubricated PA, 10% PTFE, 30% PAN Carbon Fiber Lubricated PA, Extrusion PA, Unreinforced PA, Super-Tough PA, 15% Glass Reinforced PA, 15% Glass Reinforced V-O PA, 30% Glass Reinforced PA, 30% Glass Reinforced V-O PA, 50% Glass Reinforced PA, 50% Glass and Mineral Filled PA, Molding and Extrusion Compound PA, Molding and Extrusion Compound PA, PA, Unfilled Aramid Molded Parts PA, 35% Glass Fiber Reinforced, Impact Modified PA, 40% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, and 60% Glass Fiber Reinforced PA.
Related Glossary Pages
Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C44300
Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1215 Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C85500 Glossary: Units: Pressure: Megapascal Glossary: Materials: Polymers: Polyphenylene Oxide: Alloy With Nylon, Unreinforced Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C14300 Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A285 Grade A Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 9260H Glossary: Materials: Polymers: Polystyrene: Styrene / Methyl-Methacrylate Copolymer Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C16200 Related Pages
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 30-33 ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 30-33% glass fiber reinforced}
eFunda: Glossary: Units: Fracture Toughness: Pa-Sqrt(meter)
eFunda Glossary for Units, Category:Fracture Toughness, Unit name: Pa-Sqrt(meter
eFunda Polymers: Properties of Polyamide {nylon (PA 66), copolymer}
eFunda Polymers: Properties of Polyamide {nylon (PA 66), copolymer}
eFunda Polymers: Properties of Acetal {homopolymer, chemically ...
eFunda Polymers: Properties of Acetal {homopolymer, chemically lubricated} ... State: homopolymer. Additives: chemically lubricated ...
eFunda Polymers: Properties of Polyamide {nylon (PA 612), 15% PTFE ...
eFunda Polymers: Properties of Polyamide {nylon (PA 612), 15% PTFE, 30% glass fiber reinforced, ... Coef of Thermal Expansion (10-6/ºC), 18, D696 ...
eFunda Polymers: Properties of Polycarbonate {2% silicone, 30 ...
... of Polycarbonate {2% silicone, 30% glass fiber reinforced, lubricated} ... Additives: 2% silicone, 30% glass fiber reinforced. Application: lubricated ...
eFunda Polymers: Properties of Polyamide {nylon (PA 612), 10% PTFE ...
eFunda Polymers: Properties of Polyamide {nylon (PA 612), 10% PTFE, 30% PAN carbon fiber, lubricated}
eFunda Polymers: Properties of Fluoroplastics {PTFE, 25% glass ...
eFunda Polymers: Properties of Fluoroplastics {PTFE, 25% glass fiber reinforced} ... Coef of Thermal Expansion (10-6/ºC), 77 - 100, D696 ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 30% PTFE ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 30% PTFE, lubricated} ... Coef of Thermal Expansion (10-6/ºC), 45, D696 ...
eFunda Polymers: Properties of Acetal {copolymer, 10% PAN carbon ...
... Properties of Acetal {copolymer, 10% PAN carbon fiber, 10% PTFE filled, EMI shielding (conductive)} ... Additives: 10% PAN carbon fiber, 10% PTFE filled ...
|
||||||||