13% Glass Fiber Reinforced, Heat-Stablized PA is a subcategory of Polyamide. The additative is added by weight during the manufacturing process. Its flexural modulus ranges from 700 to 750 MPa. Its tensile strength ranges from 15000 to 17000 MPa at break. Its Izod Impact strength ranges from 0.95 to 1.1 J/cm. Its elongation at break ranges from 3 to 5 %. Its specific gravity ranges from 1.21 to 1.23. Its molding pressure ranges from 7 to 20 MPa.
Polyamide, also known as PA, is a thermoplastic polycondensate. Common trade names are Ultramid and Zytel. nylon (PA 66) It has high lubricity and moderate strength. It is tough, inexpensive, but has poor dimensional stability due to water absorption (hygroscopic nature). PA is commonly used to make high-lubricity parts such as bearings, blow moldings molds, and clothing fabrics.
Additional Information
Other common Polyamide (PA) include Ceramic and Glass Fiber Reinforced PA, Molding and Extrusion Compound PA, 15% Glass Fiber Reinforced PA, 25% Glass Fiber Reinforced PA, 30-35% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 35% Glass Fiber Reinforced PA, 45% Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Mineral and Glass Fiber Reinforced PA, 40% Mineral Reinforced PA, High Impact Copolymers and Rubber Modified Compounds PA, Unfilled With Molybdenum Disulfide PA, 30% Glass Fiber Reinforced, Impact Modified PA, 30% PAN Carbon Fiber EMI Shielding (conductive) PA, PA, Heat Stabilized PA, Oil Filled PA, Plasticized PA, Type 6 / 612 Blend PA, Molding Compound PA, 15% Glass Fiber Reinforced PA, 30-33% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 60% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 15-33% Glass Fiber Reinforced, Toughened PA, 25-30% Mineral Filled, Modified High-Impact PA, Unreinforced Flame-Retardant Grade PA, 20-25% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Glass and Mineral Reinforced PA, 40-45% Mineral Filled PA, 30% Graphite Or PAN Carbon Fiber PA, 40% Aluminum Flake EMI Shielding (conductive) PA, 5% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 6% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 10% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 50% PAN Carbon Fiber EMI Shielding (conductive) PA, 30% Pitch Carbon Fiber EMI Shielding (conductive) PA, 40% Pitch Carbon Fiber EMI Shielding (conductive) PA, 15% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, 40% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, Molybdenum Disulfide Filled Antifriction PA, 5% Silicone Lubricated PA, 10% PTFE Lubricated PA, 30% PTFE Lubricated PA, 5% Molydenum Disulfide and 30% PTFE Lubricated PA, PA, Molding and Extrusion Compound PA, 30-40% Long Glass Fiber Reinforced PA, 30-40% Long Glass Fiber Reinforced PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, Molding Compound PA, 30-35% Glass Fiber Reinforced PA, 35-45% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flamed-Retardant Grade PA, 10% PTFE Lubricated PA, 15% PTFE, 30% Glass Fiber Reinforced Lubricated PA, 10% PTFE, 30% PAN Carbon Fiber Lubricated PA, Extrusion PA, Unreinforced PA, Super-Tough PA, 15% Glass Reinforced PA, 15% Glass Reinforced V-O PA, 30% Glass Reinforced PA, 30% Glass Reinforced V-O PA, 50% Glass Reinforced PA, 50% Glass and Mineral Filled PA, Molding and Extrusion Compound PA, Molding and Extrusion Compound PA, PA, Unfilled Aramid Molded Parts PA, 35% Glass Fiber Reinforced, Impact Modified PA, 40% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, and 60% Glass Fiber Reinforced PA.
Related Glossary Pages
Glossary: Materials: Polymers: Polyamide: Nylon (PA 6): 30% Long Glass Fiber Reinforced
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4718H Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A533 Type A Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C82000 Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A607 Grade 70 Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 5050 Glossary: Materials: Polymers: Cellulosic: Cellulose Acetate Propioniate: Molding and Extrusion Compound Glossary: Materials: Polymers: Polyamide: Nylon (PA 6), Semi-Aromatic Semicrystalline Copolymer: 35% Glass Fiber Reinforced Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 8642 Glossary: Materials: Alloys: Aluminum Alloy: Cast: 242.0 Related Pages
eFunda Polymers: Properties of Polyamide {nylon (PA 66), copolymer}
eFunda Polymers: Properties of Polyamide {nylon (PA 66), copolymer}
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 30-35 ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 30-35% glass fiber reinforced}
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast, heat ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast, heat stabilized} ... State: nylon (PA 6), cast. Additives: heat stabilized ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 33% glass ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 33% glass fiber reinforced, toughened}
eFunda Polymers: Properties of Polyamide {nylon (PA 66), molding ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), molding compound}
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast}
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast}
eFunda: Temper Designations of Aluminum Alloys
Applies to products which are stabilized after solution heat-treatment to carry them beyond the point of maximum strength to provide control of some special ...
eFunda Polymers: Listing of Polyphthalamide
Polyphthalamide, 45% glass reinforced, V-0. 11. Polyphthalamide, 40% glass / mineral reinforced. 12. Polyphthalamide, 40% mineral reinforced, heat stablized ...
eFunda Polymers: Properties of Polyphthalamide {40% mineral ...
eFunda Polymers: Properties of Polyphthalamide {40% mineral reinforced, heat stablized} ... Additives: 40% mineral reinforced, heat stablized ...
eFunda: Polymer (Plastic) Supplier Contact Information
Polyphthalamide, 40% mineral reinforced, heat stablized. RTP Co. 580E Front St. P.O. Box 5439. Winona, MN 55987. Toll Free: 800-433-4787 ...
|
||||||||