Polyamide: Nylon (PA 66): 30% Pitch Carbon Fiber
Home |
Directory |
Career |
News |
Industrial
|
|
|
|
Glossary » Materials » Polymers » Polyamide » Nylon (PA 66) » 30% Pitch Carbon Fiber » EMI Shielding (conductive)
30% Pitch Carbon Fiber EMI Shielding (conductive) PA is a subcategory of Polyamide. The additative is added by weight during the manufacturing process. Its elastic modulus ranges from 1400 to 2000 MPa. Its flexural modulus ranges from 1200 to 1500 MPa. Its tensile strength ranges from 15500 to 15600 MPa at break. Its flexural strength ranges from 24800 to 26000 MPa. Its Izod Impact strength ranges from 0.6 to 0.7 J/cm. Its specific gravity ranges from 1.3 to 1.31. Its coefficient of thermal expansion ranges from 16 to 19 x 10-6/°C. Its melting temperature ranges from 260 to 265 °C.
Polyamide, also known as PA, is a thermoplastic polycondensate. Common trade names are Ultramid and Zytel. nylon (PA 66) It has high lubricity and moderate strength. It is tough, inexpensive, but has poor dimensional stability due to water absorption (hygroscopic nature). PA is commonly used to make high-lubricity parts such as bearings, blow moldings molds, and clothing fabrics.
Additional Information
Other common Polyamide (PA) include Ceramic and Glass Fiber Reinforced PA, Molding and Extrusion Compound PA, 15% Glass Fiber Reinforced PA, 25% Glass Fiber Reinforced PA, 30-35% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 35% Glass Fiber Reinforced PA, 45% Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Mineral and Glass Fiber Reinforced PA, 40% Mineral Reinforced PA, High Impact Copolymers and Rubber Modified Compounds PA, Unfilled With Molybdenum Disulfide PA, 30% Glass Fiber Reinforced, Impact Modified PA, 30% PAN Carbon Fiber EMI Shielding (conductive) PA, PA, Heat Stabilized PA, Oil Filled PA, Plasticized PA, Type 6 / 612 Blend PA, Molding Compound PA, 13% Glass Fiber Reinforced, Heat-Stablized PA, 15% Glass Fiber Reinforced PA, 30-33% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 60% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 15-33% Glass Fiber Reinforced, Toughened PA, 25-30% Mineral Filled, Modified High-Impact PA, Unreinforced Flame-Retardant Grade PA, 20-25% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Glass and Mineral Reinforced PA, 40-45% Mineral Filled PA, 30% Graphite Or PAN Carbon Fiber PA, 40% Aluminum Flake EMI Shielding (conductive) PA, 5% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 6% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 10% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 50% PAN Carbon Fiber EMI Shielding (conductive) PA, 40% Pitch Carbon Fiber EMI Shielding (conductive) PA, 15% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, 40% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, Molybdenum Disulfide Filled Antifriction PA, 5% Silicone Lubricated PA, 10% PTFE Lubricated PA, 30% PTFE Lubricated PA, 5% Molydenum Disulfide and 30% PTFE Lubricated PA, PA, Molding and Extrusion Compound PA, 30-40% Long Glass Fiber Reinforced PA, 30-40% Long Glass Fiber Reinforced PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, Molding Compound PA, 30-35% Glass Fiber Reinforced PA, 35-45% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flamed-Retardant Grade PA, 10% PTFE Lubricated PA, 15% PTFE, 30% Glass Fiber Reinforced Lubricated PA, 10% PTFE, 30% PAN Carbon Fiber Lubricated PA, Extrusion PA, Unreinforced PA, Super-Tough PA, 15% Glass Reinforced PA, 15% Glass Reinforced V-O PA, 30% Glass Reinforced PA, 30% Glass Reinforced V-O PA, 50% Glass Reinforced PA, 50% Glass and Mineral Filled PA, Molding and Extrusion Compound PA, Molding and Extrusion Compound PA, PA, Unfilled Aramid Molded Parts PA, 35% Glass Fiber Reinforced, Impact Modified PA, 40% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, and 60% Glass Fiber Reinforced PA.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4427
Glossary: Materials: Polymers: Fluoroplastics: Poly(chloro-Trifluoro-Ethylene) Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C95800 Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A633 Grade E Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C14310 Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1042 Glossary: Materials: Alloys: Titanium Alloy: Wrought: Ti-3Al-8V-6Cr-4Mo-4Zr Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 52100 Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A724 Grade A Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 430FSe Related Pages
eFunda Polymers: Properties of Polycarbonate {20% PAN carbon fiber ...
... of Polycarbonate {20% PAN carbon fiber, EMI shielding (conductive)} ... Additives: 20% PAN carbon fiber. Application: EMI shielding (conductive) ...
eFunda Polymers: Properties of Polyetherimide {30% carbon fiber ...
... Properties of Polyetherimide {30% carbon fiber, EMI shielding (conductive)} ... Additives: 30% carbon fiber. Application: EMI shielding (conductive) ...
eFunda Polymers: Properties of ABS {10% stainless steel fiber, EMI ...
... of ABS {10% stainless steel fiber, EMI shielding (conductive)} ... Additives
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 33% glass ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 33% glass fiber reinforced, toughened}
eFunda: Listing of Common Polymers (Plastics) in Chronological Order
It is tough, inexpensive, and has poor dimensional stability due to water absorption (hygroscopic nature). -, Trade Name: Ultramid, Zytel. ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 30-33 ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 30-33% glass fiber reinforced}
eFunda Polymers: Properties of Polyamide {nylon (PA 66), molding ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), molding compound}
eFunda Polymers: Properties of Polyamide {nylon (PA 66), copolymer}
eFunda Polymers: Properties of Polyamide {nylon (PA 66), copolymer}
eFunda Polymers: Properties of Polyphenylene Sulfide {60 ...
... of Polyphenylene Sulfide {60% stainless steel, EMI shielding (conductive)} ... Additives: 60% stainless steel. Application: EMI shielding (conductive) ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 30% pitch ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 30% pitch carbon fiber, EMI shielding (conductive)} ... Additives: 30% pitch carbon fiber ...
|
||||||||