40% Aluminum Flake EMI Shielding (conductive) PA is a subcategory of Polyamide. The additative is added by weight during the manufacturing process. Its molding pressure ranges from 10 to 20 MPa.
Polyamide, also known as PA, is a thermoplastic polycondensate. Common trade names are Ultramid and Zytel. nylon (PA 66) It has high lubricity and moderate strength. It is tough, inexpensive, but has poor dimensional stability due to water absorption (hygroscopic nature). PA is commonly used to make high-lubricity parts such as bearings, blow moldings molds, and clothing fabrics.
Additional Information
Other common Polyamide (PA) include Ceramic and Glass Fiber Reinforced PA, Molding and Extrusion Compound PA, 15% Glass Fiber Reinforced PA, 25% Glass Fiber Reinforced PA, 30-35% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 35% Glass Fiber Reinforced PA, 45% Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Mineral and Glass Fiber Reinforced PA, 40% Mineral Reinforced PA, High Impact Copolymers and Rubber Modified Compounds PA, Unfilled With Molybdenum Disulfide PA, 30% Glass Fiber Reinforced, Impact Modified PA, 30% PAN Carbon Fiber EMI Shielding (conductive) PA, PA, Heat Stabilized PA, Oil Filled PA, Plasticized PA, Type 6 / 612 Blend PA, Molding Compound PA, 13% Glass Fiber Reinforced, Heat-Stablized PA, 15% Glass Fiber Reinforced PA, 30-33% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 60% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 15-33% Glass Fiber Reinforced, Toughened PA, 25-30% Mineral Filled, Modified High-Impact PA, Unreinforced Flame-Retardant Grade PA, 20-25% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Glass and Mineral Reinforced PA, 40-45% Mineral Filled PA, 30% Graphite Or PAN Carbon Fiber PA, 5% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 6% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 10% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 50% PAN Carbon Fiber EMI Shielding (conductive) PA, 30% Pitch Carbon Fiber EMI Shielding (conductive) PA, 40% Pitch Carbon Fiber EMI Shielding (conductive) PA, 15% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, 40% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, Molybdenum Disulfide Filled Antifriction PA, 5% Silicone Lubricated PA, 10% PTFE Lubricated PA, 30% PTFE Lubricated PA, 5% Molydenum Disulfide and 30% PTFE Lubricated PA, PA, Molding and Extrusion Compound PA, 30-40% Long Glass Fiber Reinforced PA, 30-40% Long Glass Fiber Reinforced PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, Molding Compound PA, 30-35% Glass Fiber Reinforced PA, 35-45% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flamed-Retardant Grade PA, 10% PTFE Lubricated PA, 15% PTFE, 30% Glass Fiber Reinforced Lubricated PA, 10% PTFE, 30% PAN Carbon Fiber Lubricated PA, Extrusion PA, Unreinforced PA, Super-Tough PA, 15% Glass Reinforced PA, 15% Glass Reinforced V-O PA, 30% Glass Reinforced PA, 30% Glass Reinforced V-O PA, 50% Glass Reinforced PA, 50% Glass and Mineral Filled PA, Molding and Extrusion Compound PA, Molding and Extrusion Compound PA, PA, Unfilled Aramid Molded Parts PA, 35% Glass Fiber Reinforced, Impact Modified PA, 40% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, and 60% Glass Fiber Reinforced PA.
Related Glossary Pages
Glossary: Materials: Polymers: Polyamide: Nylon (PA 6): Unfilled With Molybdenum Disulfide
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 3140 Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4135 Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4427 Glossary: Materials: Polymers: Polyester: Wholly Aromatic (liquid Crystal): Unfilled: Platable Grade Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 309S Glossary: Materials: Polymers: Fluoroplastics: Perfluoro-Alkoxyalkane (PFA) Glossary: Materials: Polymers: Thermoplastic Elastomers: Polyether/amide Block Copolymer Glossary: Materials: Polymers: Polyvinylchloride: PVC and PVC-AMC: Sheets, Rods and Tubes; Rigid Glossary: Materials: Alloys: Steel: Carbon Steel: AISI M1015 Related Pages
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast}
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast}
eFunda Polymers: Properties of Polyester (thermoset) {EMI ...
eFunda Polymers: Properties of Polyester (thermoset) {EMI shielding (conductive)
eFunda Polymers: Listing of Polyamide-imide
eFunda Polymers: Listing of Polyamide-imide. ... Polyamide-imide, unfilled, compression and injection molding compound. 2. Polyamide-imide, 30% glass fiber ...
eFunda Polymers: Listing of Acrylonitrile-Butadiene-Styrene ...
ABS, 40% long glass fiber reinforced, injection molding grade. 16. ABS, 6% stainless steel fiber, ... ABS, 40% aluminum flake, EMI shielding (conductive). ...
eFunda: Listing of Common Polymers (Plastics) in Chronological Order
It is tough, inexpensive, and has poor dimensional stability due to water absorption (hygroscopic nature). -, Trade Name: Ultramid, Zytel. ...
eFunda: Polymer (Plastic) Supplier Contact Information
ABS, 40% aluminum flake, EMI shielding (conductive). ComAlloy International Co. 481 Allied Dr. Nashville, TN 37211. Phone: 615-333-3453. FAX: 615-834-9941 ...
eFunda Polymers: Properties of ABS {7% stainless steel fiber, EMI ...
eFunda Polymers: Properties of ABS {7% stainless steel fiber, EMI shielding (
eFunda Polymers: Listing of Polyphenylene Oxide (Ashley)
Polyphenylene Oxide (modified), alloy with polystyrene, 40% aluminium flake, EMI shielding (conductive). 10. Polyphenylene Oxide (modified), alloy with ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 33% glass ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 33% glass fiber reinforced, toughened}
eFunda Polymers: Properties of Polyetherimide {30% carbon fiber ...
... Properties of Polyetherimide {30% carbon fiber, EMI shielding (conductive)} ... Additives: 30% carbon fiber. Application: EMI shielding (conductive) ...
|
||||||||