Polyamide: Nylon (PA 66): Molybdenum Disulfide Filled
Home |
Directory |
Career |
News |
Industrial
|
|
|
|
Glossary » Materials » Polymers » Polyamide » Nylon (PA 66) » Molybdenum Disulfide Filled » Antifriction
Molybdenum Disulfide Filled Antifriction PA is a subcategory of Polyamide. The additative is added during the manufacturing process. Its elastic modulus ranges from 350 to 550 MPa. Its flexural modulus ranges from 420 to 495 MPa. Its tensile strength ranges from 10500 to 13700 MPa at break. Its flexural strength ranges from 15000 to 20300 MPa. Its compressive strength ranges from 12000 to 12500 MPa. Its Izod Impact strength ranges from 0.9 to 4.5 J/cm. Its elongation at break ranges from 4.4 to 40 %. Its specific gravity ranges from 1.15 to 1.18. Its melting temperature ranges from 260 to 265 °C. Its molding pressure ranges from 5 to 25 MPa.
Polyamide, also known as PA, is a thermoplastic polycondensate. Common trade names are Ultramid and Zytel. nylon (PA 66) It has high lubricity and moderate strength. It is tough, inexpensive, but has poor dimensional stability due to water absorption (hygroscopic nature). PA is commonly used to make high-lubricity parts such as bearings, blow moldings molds, and clothing fabrics.
Additional Information
Other common Polyamide (PA) include Ceramic and Glass Fiber Reinforced PA, Molding and Extrusion Compound PA, 15% Glass Fiber Reinforced PA, 25% Glass Fiber Reinforced PA, 30-35% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 35% Glass Fiber Reinforced PA, 45% Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Mineral and Glass Fiber Reinforced PA, 40% Mineral Reinforced PA, High Impact Copolymers and Rubber Modified Compounds PA, Unfilled With Molybdenum Disulfide PA, 30% Glass Fiber Reinforced, Impact Modified PA, 30% PAN Carbon Fiber EMI Shielding (conductive) PA, PA, Heat Stabilized PA, Oil Filled PA, Plasticized PA, Type 6 / 612 Blend PA, Molding Compound PA, 13% Glass Fiber Reinforced, Heat-Stablized PA, 15% Glass Fiber Reinforced PA, 30-33% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 60% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 15-33% Glass Fiber Reinforced, Toughened PA, 25-30% Mineral Filled, Modified High-Impact PA, Unreinforced Flame-Retardant Grade PA, 20-25% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Glass and Mineral Reinforced PA, 40-45% Mineral Filled PA, 30% Graphite Or PAN Carbon Fiber PA, 40% Aluminum Flake EMI Shielding (conductive) PA, 5% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 6% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 10% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 50% PAN Carbon Fiber EMI Shielding (conductive) PA, 30% Pitch Carbon Fiber EMI Shielding (conductive) PA, 40% Pitch Carbon Fiber EMI Shielding (conductive) PA, 15% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, 40% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, 5% Silicone Lubricated PA, 10% PTFE Lubricated PA, 30% PTFE Lubricated PA, 5% Molydenum Disulfide and 30% PTFE Lubricated PA, PA, Molding and Extrusion Compound PA, 30-40% Long Glass Fiber Reinforced PA, 30-40% Long Glass Fiber Reinforced PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, Molding Compound PA, 30-35% Glass Fiber Reinforced PA, 35-45% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flamed-Retardant Grade PA, 10% PTFE Lubricated PA, 15% PTFE, 30% Glass Fiber Reinforced Lubricated PA, 10% PTFE, 30% PAN Carbon Fiber Lubricated PA, Extrusion PA, Unreinforced PA, Super-Tough PA, 15% Glass Reinforced PA, 15% Glass Reinforced V-O PA, 30% Glass Reinforced PA, 30% Glass Reinforced V-O PA, 50% Glass Reinforced PA, 50% Glass and Mineral Filled PA, Molding and Extrusion Compound PA, Molding and Extrusion Compound PA, PA, Unfilled Aramid Molded Parts PA, 35% Glass Fiber Reinforced, Impact Modified PA, 40% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, and 60% Glass Fiber Reinforced PA.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 50B50H
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 8650H Glossary: Materials: Polymers: Polyester: Wholly Aromatic (liquid Crystal): Unfilled: Medium Melting Point Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C81800 Glossary: Design: Oring: Material: Vamac Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A514 Type K Glossary: Materials: Polymers: Polyamide: Nylon (PA 612): 10% PTFE, 30% PAN Carbon Fiber: Lubricated Glossary: Materials: Polymers: Polyacetal: Homopolymer: 21% PTFE Filled Glossary: Materials: Polymers: Polystyrene: Styrene / Maleic Anhydride (SMA) Copolymer: Molding and Extrusion Glossary: Materials: Alloys: Steel: Stainless Steel: AM-350 Related Pages
eFunda Polymers: Listing of Polyamide (Ultramid, Zytel)
Polyamide, also known as PA, or Nylon, has been mass-produced since 1935. ... Polyamide, nylon alloys, ceramic and glass fiber reinforced. ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 30-35 ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 30-35% glass fiber reinforced}
eFunda Polymers: Properties of Polyamide {nylon (PA 66 ...
... Properties of Polyamide {nylon (PA 66), molybdenum disulfide filled, antifriction} ... Additives: molybdenum disulfide filled. Application: antifriction ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 30-33 ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 30-33% glass fiber reinforced}
eFunda Polymers: Properties of Polyamide {nylon (PA 66 ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), unreinforced, flame-
eFunda Polymers: Properties of Polyamide {nylon (PA 66), molding ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), molding compound}
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 33% glass ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 33% glass fiber reinforced, toughened}
Antifriction Bearings
Introduction to rolling contact bearings which require very little friction for low differential surface speeds.
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast, Type ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast, Type 6 / 612 blend
eFunda: Listing of Common Polymers (Plastics) in Chronological Order
It is tough, inexpensive, and has poor dimensional stability due to water absorption (hygroscopic nature). -, Trade Name: Ultramid, Zytel. ...
|
||||||||