PA is a subcategory of Polyamide. Its elastic modulus ranges from 150 to 410 MPa. Its flexural modulus ranges from 150 to 410 MPa. Its tensile strength ranges from 7400 to 12400 MPa at break. Its elongation at break ranges from 40 to 150 %. Its hardness ranges from 114 to 119 Rockwell R. Its specific gravity ranges from 1.08 to 1.14. Its melting temperature ranges from 200 to 255 °C. Its molding pressure ranges from 1 to 15 MPa.
Polyamide, also known as PA, is a thermoplastic polycondensate. Common trade names are Ultramid and Zytel. nylon (PA 66), copolymer It has high lubricity and moderate strength. It is tough, inexpensive, but has poor dimensional stability due to water absorption (hygroscopic nature). PA is commonly used to make high-lubricity parts such as bearings, blow moldings molds, and clothing fabrics.
Additional Information
Other common Polyamide (PA) include Ceramic and Glass Fiber Reinforced PA, Molding and Extrusion Compound PA, 15% Glass Fiber Reinforced PA, 25% Glass Fiber Reinforced PA, 30-35% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 35% Glass Fiber Reinforced PA, 45% Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Mineral and Glass Fiber Reinforced PA, 40% Mineral Reinforced PA, High Impact Copolymers and Rubber Modified Compounds PA, Unfilled With Molybdenum Disulfide PA, 30% Glass Fiber Reinforced, Impact Modified PA, 30% PAN Carbon Fiber EMI Shielding (conductive) PA, PA, Heat Stabilized PA, Oil Filled PA, Plasticized PA, Type 6 / 612 Blend PA, Molding Compound PA, 13% Glass Fiber Reinforced, Heat-Stablized PA, 15% Glass Fiber Reinforced PA, 30-33% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 60% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 15-33% Glass Fiber Reinforced, Toughened PA, 25-30% Mineral Filled, Modified High-Impact PA, Unreinforced Flame-Retardant Grade PA, 20-25% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Glass and Mineral Reinforced PA, 40-45% Mineral Filled PA, 30% Graphite Or PAN Carbon Fiber PA, 40% Aluminum Flake EMI Shielding (conductive) PA, 5% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 6% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 10% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 50% PAN Carbon Fiber EMI Shielding (conductive) PA, 30% Pitch Carbon Fiber EMI Shielding (conductive) PA, 40% Pitch Carbon Fiber EMI Shielding (conductive) PA, 15% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, 40% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, Molybdenum Disulfide Filled Antifriction PA, 5% Silicone Lubricated PA, 10% PTFE Lubricated PA, 30% PTFE Lubricated PA, 5% Molydenum Disulfide and 30% PTFE Lubricated PA, Molding and Extrusion Compound PA, 30-40% Long Glass Fiber Reinforced PA, 30-40% Long Glass Fiber Reinforced PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, Molding Compound PA, 30-35% Glass Fiber Reinforced PA, 35-45% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flamed-Retardant Grade PA, 10% PTFE Lubricated PA, 15% PTFE, 30% Glass Fiber Reinforced Lubricated PA, 10% PTFE, 30% PAN Carbon Fiber Lubricated PA, Extrusion PA, Unreinforced PA, Super-Tough PA, 15% Glass Reinforced PA, 15% Glass Reinforced V-O PA, 30% Glass Reinforced PA, 30% Glass Reinforced V-O PA, 50% Glass Reinforced PA, 50% Glass and Mineral Filled PA, Molding and Extrusion Compound PA, Molding and Extrusion Compound PA, PA, Unfilled Aramid Molded Parts PA, 35% Glass Fiber Reinforced, Impact Modified PA, 40% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, and 60% Glass Fiber Reinforced PA.
Related Glossary Pages
Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C17200
Glossary: Materials: Polymers: Polyamide: Nylon (PA 6), Cast: Type 6 / 612 Blend Glossary: Materials: Alloys: Steel: Tool Steel: AISI M34 Glossary: Materials: Alloys: Copper Alloy: Wire: AWG-37 Glossary: Materials: Alloys: Magnesium Alloy: ASTM ZK51A-T5 Glossary: Materials: Alloys: Magnesium Alloy: ASTM AZ31B-F Glossary: Materials: Alloys: Steel: Stainless Steel: 904L Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C11100 Glossary: Materials: Polymers: Polyaryletherketone: Poly(etherether-Ketone): Unfilled Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A514 Type J Related Pages
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast, plasticized}
eFunda Polymers: Properties of Polyamide {nylon (PA 66), molding ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), molding compound}
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 33% glass ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 33% glass fiber reinforced, toughened}
eFunda: Engineering Materials
Home page for properties of materials such as elements, alloys, polymers, and piezo ceramics.
eFunda Polymers: Properties of Polyamide {nylon (PA 66), copolymer}
eFunda Polymers: Properties of Polyamide {nylon (PA 66), copolymer}
eFunda: Polymer (Plastic) Home Page
Index page for polymers. ... General Information. Polymer Home. Glossary. Material Science. Overview · Characteristics · Comparisons. Selection Criteria ...
eFunda: Polymer (Plastic) Supplier Contact Information
Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219. Phone: 718-851-8111 ... Bamberger Polymers, Inc. 2 Jericho Plaza. Jericho, NY 11753 ...
eFunda: Piezo Material Data
Select specific piezoelectric material to view constitutive properties.
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 15-33 ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 15-33% glass fiber reinforced, toughened}
eFunda: Pressure Unit Category
kip/in, ksi, KSI, 6.89476x106 Pa ... mmHg, torr, Torr (0 °C), 133.322 Pa. ·, millimeter of water (15.56°C) · mmH2O, mmCE (15.56 °C), 9.79706 Pa ...
|
||||||||