Polyamide: Nylon (PA 6), Cast: Type 6 / 612 Blend
Home |
Directory |
Career |
News |
Industrial
|
|
|
|
Glossary » Materials » Polymers » Polyamide » Type 6 / 612 Blend
Type 6 / 612 Blend PA is a subcategory of Polyamide. The additative is added during the manufacturing process. Its elastic modulus ranges from 240 to 330 MPa. Its flexural modulus ranges from 285 to 385 MPa. Its tensile strength ranges from 8700 to 11500 MPa at break. Its flexural strength ranges from 15000 to 20000 MPa. Its Izod Impact strength ranges from 0.9 to 1.4 J/cm. Its elongation at break ranges from 25 to 80 %. Its hardness ranges from 100 to 115 . Its specific gravity ranges from 1.1 to 1.13. Its coefficient of thermal expansion ranges from 45 to 45 x 10-6/°C. Its melting temperature ranges from 227 to 238 °C.
Polyamide, also known as PA, is a thermoplastic polycondensate. Common trade names are Ultramid and Zytel. nylon (PA 6), cast It has high lubricity and moderate strength. It is tough, inexpensive, but has poor dimensional stability due to water absorption (hygroscopic nature). PA is commonly used to make high-lubricity parts such as bearings, blow moldings molds, and clothing fabrics.
Additional Information
Other common Polyamide (PA) include Ceramic and Glass Fiber Reinforced PA, Molding and Extrusion Compound PA, 15% Glass Fiber Reinforced PA, 25% Glass Fiber Reinforced PA, 30-35% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 35% Glass Fiber Reinforced PA, 45% Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Mineral and Glass Fiber Reinforced PA, 40% Mineral Reinforced PA, High Impact Copolymers and Rubber Modified Compounds PA, Unfilled With Molybdenum Disulfide PA, 30% Glass Fiber Reinforced, Impact Modified PA, 30% PAN Carbon Fiber EMI Shielding (conductive) PA, PA, Heat Stabilized PA, Oil Filled PA, Plasticized PA, Molding Compound PA, 13% Glass Fiber Reinforced, Heat-Stablized PA, 15% Glass Fiber Reinforced PA, 30-33% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 60% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 15-33% Glass Fiber Reinforced, Toughened PA, 25-30% Mineral Filled, Modified High-Impact PA, Unreinforced Flame-Retardant Grade PA, 20-25% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Glass and Mineral Reinforced PA, 40-45% Mineral Filled PA, 30% Graphite Or PAN Carbon Fiber PA, 40% Aluminum Flake EMI Shielding (conductive) PA, 5% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 6% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 10% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 50% PAN Carbon Fiber EMI Shielding (conductive) PA, 30% Pitch Carbon Fiber EMI Shielding (conductive) PA, 40% Pitch Carbon Fiber EMI Shielding (conductive) PA, 15% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, 40% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, Molybdenum Disulfide Filled Antifriction PA, 5% Silicone Lubricated PA, 10% PTFE Lubricated PA, 30% PTFE Lubricated PA, 5% Molydenum Disulfide and 30% PTFE Lubricated PA, PA, Molding and Extrusion Compound PA, 30-40% Long Glass Fiber Reinforced PA, 30-40% Long Glass Fiber Reinforced PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, Molding Compound PA, 30-35% Glass Fiber Reinforced PA, 35-45% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flamed-Retardant Grade PA, 10% PTFE Lubricated PA, 15% PTFE, 30% Glass Fiber Reinforced Lubricated PA, 10% PTFE, 30% PAN Carbon Fiber Lubricated PA, Extrusion PA, Unreinforced PA, Super-Tough PA, 15% Glass Reinforced PA, 15% Glass Reinforced V-O PA, 30% Glass Reinforced PA, 30% Glass Reinforced V-O PA, 50% Glass Reinforced PA, 50% Glass and Mineral Filled PA, Molding and Extrusion Compound PA, Molding and Extrusion Compound PA, PA, Unfilled Aramid Molded Parts PA, 35% Glass Fiber Reinforced, Impact Modified PA, 40% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, and 60% Glass Fiber Reinforced PA.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A302 Grade B
Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 304LN Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4130H Glossary: Materials: Polymers: Polyamide: Nylon (PA 6): 40% Mineral and Glass Fiber Reinforced Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 8645 Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 422 Glossary: Materials: Alloys: Aluminum Alloy: Cast: 296.0 Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 202 Glossary: Design: Oring: Material: Silicone Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 442 Related Pages
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast}
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast}
eFunda: Glossary of Polymers (Plastics)
Common terms used in material science of polymers.
eFunda Polymers: Properties of Polyamide {nylon (PA 66 ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), unreinforced, flame-
eFunda Polymers: Properties of Polyamide {nylon (PA 66), molding ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), molding compound}
eFunda: Polymer (Plastic) Supplier Contact Information
American Polymers, Inc. 53 Millbrook St. P.O. Box 60398. Worcester, MA 01606 ... Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219 ...
eFunda: Listing of Common Polymers (Plastics) in Chronological Order
It is tough, inexpensive, and has poor dimensional stability due to water absorption (hygroscopic nature). -, Trade Name: Ultramid, Zytel. ...
eFunda: Glossary: Materials: Alloys: Copper Alloy: UNS C95500
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast, Type 6 / 612 blend
eFunda: Glossary: Materials: Alloys: Aluminum Alloy: 356.0
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast, Type 6 / 612 blend
eFunda: Glossary: Units: Fracture Toughness: Pa-Sqrt(meter)
eFunda Glossary for Units, Category:Fracture Toughness, Unit name: Pa-Sqrt(meter
eFunda: Glossary: Materials: Alloys: Aluminum Alloy: 384.0
eFunda Polymers: Properties of Polyamide {nylon (PA 6), cast, Type 6 / 612 blend
|
||||||||