45% Glass Fiber Reinforced PA is a subcategory of Polyamide. The additative is added by weight during the manufacturing process. Its tensile strength ranges from 33500 to 35500 MPa at break. Its elongation at break ranges from 2.2 to 2.2 %. Its coefficient of thermal expansion ranges from 15 to 48 x 10-6/°C. Its molding pressure ranges from 5 to 20 MPa.
Polyamide, also known as PA, is a thermoplastic polycondensate. Common trade names are Ultramid and Zytel. nylon (PA 6), semi-aromatic semicrystalline copolymer It has high lubricity and moderate strength. It is tough, inexpensive, but has poor dimensional stability due to water absorption (hygroscopic nature). PA is commonly used to make high-lubricity parts such as bearings, blow moldings molds, and clothing fabrics.
Additional Information
Other common Polyamide (PA) include Ceramic and Glass Fiber Reinforced PA, Molding and Extrusion Compound PA, 15% Glass Fiber Reinforced PA, 25% Glass Fiber Reinforced PA, 30-35% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 35% Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Mineral and Glass Fiber Reinforced PA, 40% Mineral Reinforced PA, High Impact Copolymers and Rubber Modified Compounds PA, Unfilled With Molybdenum Disulfide PA, 30% Glass Fiber Reinforced, Impact Modified PA, 30% PAN Carbon Fiber EMI Shielding (conductive) PA, PA, Heat Stabilized PA, Oil Filled PA, Plasticized PA, Type 6 / 612 Blend PA, Molding Compound PA, 13% Glass Fiber Reinforced, Heat-Stablized PA, 15% Glass Fiber Reinforced PA, 30-33% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, 30% Long Glass Fiber Reinforced PA, 40% Long Glass Fiber Reinforced PA, 50% Long Glass Fiber Reinforced PA, 60% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 15-33% Glass Fiber Reinforced, Toughened PA, 25-30% Mineral Filled, Modified High-Impact PA, Unreinforced Flame-Retardant Grade PA, 20-25% Glass Fiber Reinforced Flame-Retardant Grade PA, 40% Glass and Mineral Reinforced PA, 40-45% Mineral Filled PA, 30% Graphite Or PAN Carbon Fiber PA, 40% Aluminum Flake EMI Shielding (conductive) PA, 5% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 6% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 10% Stainless Steel, Long Fiber EMI Shielding (conductive) PA, 50% PAN Carbon Fiber EMI Shielding (conductive) PA, 30% Pitch Carbon Fiber EMI Shielding (conductive) PA, 40% Pitch Carbon Fiber EMI Shielding (conductive) PA, 15% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, 40% Nickel Coated Carbon Fiber EMI Shielding (conductive) PA, Molybdenum Disulfide Filled Antifriction PA, 5% Silicone Lubricated PA, 10% PTFE Lubricated PA, 30% PTFE Lubricated PA, 5% Molydenum Disulfide and 30% PTFE Lubricated PA, PA, Molding and Extrusion Compound PA, 30-40% Long Glass Fiber Reinforced PA, 30-40% Long Glass Fiber Reinforced PA, 30% Glass Fiber Reinforced Flame-Retardant Grade PA, Molding Compound PA, 30-35% Glass Fiber Reinforced PA, 35-45% Long Glass Fiber Reinforced PA, Unreinforced, Toughened PA, 33% Glass Fiber Reinforced, Toughened PA, 30% Glass Fiber Reinforced Flamed-Retardant Grade PA, 10% PTFE Lubricated PA, 15% PTFE, 30% Glass Fiber Reinforced Lubricated PA, 10% PTFE, 30% PAN Carbon Fiber Lubricated PA, Extrusion PA, Unreinforced PA, Super-Tough PA, 15% Glass Reinforced PA, 15% Glass Reinforced V-O PA, 30% Glass Reinforced PA, 30% Glass Reinforced V-O PA, 50% Glass Reinforced PA, 50% Glass and Mineral Filled PA, Molding and Extrusion Compound PA, Molding and Extrusion Compound PA, PA, Unfilled Aramid Molded Parts PA, 35% Glass Fiber Reinforced, Impact Modified PA, 40% Glass Fiber Reinforced PA, 50% Glass Fiber Reinforced PA, and 60% Glass Fiber Reinforced PA.
Related Glossary Pages
Glossary: Materials: Polymers: Thermoplastic Elastomers: Block Copolymer of Styrene and Butadiene Or Styrene and Isoprene
Glossary: Materials: Alloys: Steel: Tool Steel: AISI W5 Glossary: Units: Pressure: Millibar Glossary: Materials: Polymers: Polyamide: Nylon (PA 6), Cast Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 8720 Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C17200 Glossary: Units: Pressure: Millimeter of Water (4°C) Glossary: Materials: Polymers: Polyacrylates: Multipolymer: Molding and Extrusion Compounds Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A734 Type B Glossary: Materials: Polymers: Polyphenylene Sulfide: 30% Glass Fiber Reinforced Related Pages
eFunda Polymers: Properties of Polyamide {nylon (PA 612), 35-45 ...
... Properties of Polyamide {nylon (PA 612), 35-45% long glass fiber reinforced} ... State: nylon (PA 612). Additives: 35-45% long glass fiber reinforced ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 30-35 ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 30-35% glass fiber reinforced}
eFunda: Glossary: Units: Fracture Toughness: Pa-Sqrt(meter)
eFunda Glossary for Units, Category:Fracture Toughness, Unit name: Pa-Sqrt(meter
eFunda Polymers: Properties of Polyester / alkyd, thermoset {vinyl ...
State: vinyl ester. Additives: glass fiber reinforced. Application: BMC ... Hardness, 45 - 65, Barcol, D638. Izod Impact (J/cm of notch) ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), molding ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), molding and extrusion compound}
eFunda Polymers: Properties of Polyamide {nylon (PA 66 ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), unreinforced, flame-
eFunda: Polymer (Plastic) Home Page
Index page for polymers. ... General Information. Polymer Home. Glossary. Material Science. Overview · Characteristics · Comparisons. Selection Criteria ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 30-33 ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 30-33% glass fiber reinforced}
eFunda Polymers: Properties of Polypropylene {homopolymer, 10 - 30 ...
State: homopolymer. Additives: 10 - 30% glass fiber reinforced ... at yield or break, 45 - 58, D695. Flexural Strength (MPa) at yield or break, 49 - 138 ...
eFunda: Polymer (Plastic) Supplier Contact Information
Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219. Phone: 718-851-8111
|
||||||||