Polyaryletherketone: Poly(arylether-Ketone): Modified, 40% Glass
Home |
Directory |
Career |
News |
Industrial
|
|
|
|
Glossary » Materials » Polymers » Polyaryletherketone » Modified, 40% Glass
Modified, 40% Glass PAEK is a subcategory of Polyaryletherketone. The additative is added by weight during the manufacturing process. Its molding pressure ranges from 10 to 20 MPa.
Polyaryletherketone, also known as PAEK, is a thermoplastic polycondensate. poly(arylether-ketone) It provides high performance with excelent high-temperature properties. Its applications include airplane and automobile parts, chemical plants, oil, gas, and steam processing equipments.
Additional Information
Other common Polyaryletherketone (PAEK) include Unfilled PAEK, 30% Glass Fiber Reinforced PAEK, 40% Glass Fiber Reinforced PAEK, 30% Carbon Fiber PAEK, Unfilled PAEK, 30% Glass Fiber Reinforced PAEK, and 30% Carbon Fiber Reinforced PAEK.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A611 Grade C
Glossary: Materials: Polymers: Polyacetal: Copolymer: 2 - 20% PTFE Filled Glossary: Materials: Alloys: Titanium Alloy: Wrought Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4032H Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1566 Glossary: Materials: Alloys: Aluminum Alloy: Cast: 514.0 Glossary: Materials: Alloys: Aluminum Alloy: Cast: 771.0 Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C95410 Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C62400 Glossary: Materials: Polymers: Polyphthalamide: 50% Glass / Mineral Reinforced, V-0 Related Pages
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 40% long ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 40% long glass fiber reinforced} ... State: nylon (PA 6). Additives: 40% long glass fiber reinforced ...
eFunda: Properties of Piezo Material Lead Zirconate Titanate (PZT-5A)
eFunda: Properties of Piezo Material Lead Zirconate Titanate (PZT-5A)
eFunda: Estimanation of Lamina Material Constants
Calculates the equivalent material constants for a fiber reinforced composite lamina.
Modified Bessel Function
Modified Bessel's differential equation, Bessel functions, their properties, and some special results as well as Hankel functions.
eFunda Polymers: Properties of Sulfone polymers {modified ...
eFunda Polymers: Properties of Sulfone polymers {modified polysulfone, mineral filled}
eFunda: Polymer (Plastic) Supplier Contact Information
Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219. Phone: 718-851-8111
eFunda Polymers: Properties of Polyphthalamide {40% glass ...
eFunda Polymers: Properties of Polyphthalamide {40% glass / mineral reinforced, heat stablized}
eFunda Polymers: Properties of Polycarbonate {polycarbonate ...
... Properties of Polycarbonate {polycarbonate / polyester blends, impact modified} ... Additives: polycarbonate / polyester blends, impact modified ...
eFunda: Listing of Common Polymers (Plastics)
Polyaryletherketone, (PAEK), (Ketone), Thermoplastic polycondensate. Polybutadiene, (PBD), Thermoplastic polymer. Polybutylene, (PB), Thermoplastic polymer. ...
eFunda: Engineering Materials
Home page for properties of materials such as elements, alloys, polymers, and piezo ceramics.
|
||||||||