Polyaryletherketone: Poly(etherether-Ketone): 30% Glass Fiber Reinforced
Home |
Directory |
Career |
News |
Industrial
|
|
|
|
Glossary » Materials » Polymers » Polyaryletherketone » 30% Glass Fiber Reinforced
30% Glass Fiber Reinforced PAEK is a subcategory of Polyaryletherketone. The additative is added by weight during the manufacturing process. Its elastic modulus ranges from 1250 to 1600 MPa. Its tensile strength ranges from 22500 to 28500 MPa at break. Its flexural strength ranges from 33000 to 42000 MPa. Its compressive strength ranges from 21300 to 22400 MPa. Its Izod Impact strength ranges from 2.1 to 2.7 J/cm. Its elongation at break ranges from 2 to 3 %. Its specific gravity ranges from 1.49 to 1.54. Its molding pressure ranges from 10 to 20 MPa.
Polyaryletherketone, also known as PAEK, is a thermoplastic polycondensate. poly(etherether-ketone) It provides high performance with excelent high-temperature properties. Its applications include airplane and automobile parts, chemical plants, oil, gas, and steam processing equipments.
Additional Information
Other common Polyaryletherketone (PAEK) include Unfilled PAEK, 30% Glass Fiber Reinforced PAEK, 40% Glass Fiber Reinforced PAEK, Modified, 40% Glass PAEK, 30% Carbon Fiber PAEK, Unfilled PAEK, and 30% Carbon Fiber Reinforced PAEK.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A514 Type N
Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C80100 Glossary: Materials: Alloys: Steel: Stainless Steel: AISI S30430 Glossary: Materials: Polymers: Polystyrene: Copolymer: 20% PAN Carbon Fiber: EMI Shielding (conductive) Glossary: Materials: Alloys: Magnesium Alloy: ASTM AZ91C-T6 Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 316LN Glossary: Materials: Polymers: Polyacetal: Homopolymer: UV Stabilized, 20% Glass Filled Glossary: Materials: Polymers: Polyphenylene Oxide: Alloy With Polystyrene, 40% Aluminium Flake: EMI Shielding (conductive) Glossary: Materials: Polymers: Polyphenylene Sulfide: 30% Glass Fiber, 15% PTFE Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 430Ti Related Pages
eFunda Polymers: Properties of Polycarbonate {20 - 30% long glass ...
eFunda Polymers: Properties of Polycarbonate {20 - 30% long glass fiber reinforced} ... Additives: 20 - 30% long glass fiber reinforced ...
eFunda Polymers: Properties of Polypropylene {homopolymer, 20 - 30 ...
... Properties of Polypropylene {homopolymer, 20 - 30% long glass fiber reinforced} ... State: homopolymer. Additives: 20 - 30% long glass fiber reinforced ...
eFunda: Glossary of Polymers (Plastics)
Common terms used in material science of polymers.
eFunda: Listing of Common Polymers (Plastics) in Chronological Order
eFunda: Listing of Common Polymers (Plastics) in Chronological Order. ... The first volume-produced synthesized polymer resin, PF was used in early consumer ...
eFunda Polymers: Properties of Polyamide {nylon (PA 610), 30 ...
Trade Publications. Reinforced Plastics · Design-2-Part · Chemical Processing ... Additives: 30% glass fiber reinforced. Application: flame-retardant grade ...
eFunda Polymers: Properties of Polyurethane {thermoplastic, 30 ...
... Properties of Polyurethane {thermoplastic, 30% long glass fiber reinforced} ... State: thermoplastic. Additives: 30% long glass fiber reinforced ...
eFunda Polymers: Properties of Polypropylene {homopolymer, 10 - 30 ...
... Polymers: Properties of Polypropylene {homopolymer, 10 - 30% glass fiber reinforced} ... State: homopolymer. Additives: 10 - 30% glass fiber reinforced ...
eFunda: Polymer (Plastic) Supplier Contact Information
Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219. Phone: 718-851-8111
eFunda: Polymers (Plastics) Sorted by Thermoplastic/Thermoset
Polyaryletherketone, (PAEK), (Ketone). •, Polybutadiene, (PBD). •, Polybutylene, (PB). •, Polycarbonate, (PC). •, Polyektone, (PK). ...
eFunda: Polymer (Plastic) Supplier Contact Information
American Polymers, Inc. 53 Millbrook St. P.O. Box 60398. Worcester, MA 01606 ... Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219 ...
|
||||||||