Polycarbonate: 10-15% PTFE, 20% Fiber Reinforced: Lubricated
Home |
Directory |
Career |
News |
Industrial
|
|
|
|
Glossary » Materials » Polymers » Polycarbonate » 10-15% PTFE, 20% Fiber Reinforced » Lubricated
10-15% PTFE, 20% Fiber Reinforced Lubricated PC is a subcategory of Polycarbonate. The additative is added by weight during the manufacturing process. Its flexural modulus ranges from 850 to 900 MPa. Its tensile strength ranges from 12000 to 15000 MPa at break. Its flexural strength ranges from 18000 to 23000 MPa. Its Izod Impact strength ranges from 1.8 to 3.5 J/cm. Its specific gravity ranges from 1.43 to 1.5. Its coefficient of thermal expansion ranges from 21.6 to 23.4 x 10-6/°C.
Polycarbonate, also known as PC, is a thermoplastic polycondensate. Common trade names are Lexan and Makrolon. It has excellent strength, toughness, dimensional stability, dielectric strength, flame retardancy, and impact resistance (highest among transparent rigid materials). It is, however, susceptible to stress cracking with aromatic solvents, and is difficult to machine. PC can be used to make optical lenses, windows, medical items, CD's, and power tool housings. It can also be used in truck cabs.
Additional Information
Other common Polycarbonate (PC) include Unfilled Molding and Extrusion Resins, High Viscosity PC, Unfilled Molding and Extrusion Resins, Low Viscosity PC, 10% Glass Fiber Reinforced PC, 30% Glass Fiber Reinforced PC, 20 - 30% Long Glass Fiber Reinforced PC, 40% Long Glass Fiber Reinforced PC, 50% Long Glass Fiber Reinforced PC, 35% Random Glass Mat PC, 20 - 30% Long Glass Fiber Reinforced Flame-Retardant Grade PC, Polyester Copolymer High Heat PC, Polycarbonate Copolymer High Heat PC, Polycarbonate / Polyester Blends, Impact Modified PC, 6% Stainless Steel Fiber Conductive PC, 10% Stainless Steel Fiber EMI Shielding (conductive) PC, 20% PAN Carbon Fiber EMI Shielding (conductive) PC, 30% PAN Carbon Fiber EMI Shielding (conductive) PC, 40% PAN Carbon Fiber EMI Shielding (conductive) PC, 10-15% PTFE Lubricated PC, 30% PTFE Lubricated PC, and 2% Silicone, 30% Glass Fiber Reinforced Lubricated PC.
Related Glossary Pages
Glossary: Materials: Alloys: Magnesium Alloy: ASTM AZ81A-T4
Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 503 Glossary: Materials: Polymers: Polyester: Glass Fiber Reinforced, Unidirectional Glass Glossary: Materials: Polymers: Polyester: Poly(ethylene-Terephthalate): Recycled Content, 30% Glass Fiber Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 15B35H Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 430Ti Glossary: Materials: Polymers: Polyamide: Nylon (PA 46): Super-Tough Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1021 Glossary: Materials: Polymers: Epoxy: Bisphenol, Low Density: Glass Sphere Filled: Molding Compounds Glossary: Materials: Polymers: Polyamide: Nylon (PA 6), Cast: Type 6 / 612 Blend Related Pages
eFunda: Convert parsec to other Length units
Symbol: pc. Category: Length. SI Equivalent: 3.08568×1016 m ... 1768.4000000000001 pc = Length. Symbol, Unit Name. 5.45671×1029, Å · angstrom ...
eFunda: Glossary: Units: Energy: Kilocalorie (15°C)
eFunda Polymers: Properties of Polycarbonate {10-15% PTFE, lubricated}. eFunda Polymers: Properties of Polycarbonate {10-15% PTFE, lubricated} ...
eFunda Polymers: Properties of Polycarbonate {copolymer ...
eFunda Polymers: Properties of Polycarbonate {copolymer, polycarbonate copolymer
eFunda Polymers: Properties of Polycarbonate {polycarbonate ...
eFunda Polymers: Properties of Polycarbonate {polycarbonate / polyester blends, impact modified}
eFunda Polymers: Properties of ABS {ABS / PC, injection molding ...
eFunda Polymers: Properties of ABS {ABS / PC, injection molding and extrusion}
eFunda: Convert parsec to other Length units
Symbol: pc. Category: Length. SI Equivalent: 3.08568×1016 m ... 1 pc = Length. Symbol, Unit Name. 5.83109×1026, a.u., a0, b · a.u. of length ...
eFunda Polymers: Properties of Polycarbonate {20% PAN carbon fiber ...
eFunda Polymers: Properties of Polycarbonate {20% PAN carbon fiber, EMI shielding (conductive)}
eFunda: Polymer (Plastic) Supplier Contact Information
Polycarbonate, 10-15% PTFE, lubricated. ComAlloy International Co. 481 Allied Dr
eFunda Polymers: Properties of Sulfone polymers {polysulfone, 20 ...
eFunda Polymers: Properties of Sulfone polymers {polysulfone, 20% glass fiber reinforced} ... State: polysulfone. Additives: 20% glass fiber reinforced ...
eFunda Polymers: Properties of ABS {20% glass fiber reinforced ...
eFunda Polymers: Properties of ABS {20% glass fiber reinforced, injection molding grade}
|
||||||||