Polycarbonate: 30% PAN Carbon Fiber: EMI Shielding (conductive)
Home |
Directory |
Career |
News |
Industrial
|
|
|
|
Glossary » Materials » Polymers » Polycarbonate » 30% PAN Carbon Fiber » EMI Shielding (conductive)
30% PAN Carbon Fiber EMI Shielding (conductive) PC is a subcategory of Polycarbonate. The additative is added by weight during the manufacturing process. Its elastic modulus ranges from 250 to 2150 MPa. Its flexural modulus ranges from 240 to 1900 MPa. Its tensile strength ranges from 20000 to 24000 MPa at break. Its flexural strength ranges from 30000 to 36000 MPa. Its compressive strength ranges from 19000 to 26000 MPa. Its elongation at break ranges from 1 to 5 %. Its hardness ranges from 118 to 119 Rockwell R. Its specific gravity ranges from 1.32 to 1.33. Its melting temperature ranges from 149 to 150 °C. Its molding pressure ranges from 15 to 20 MPa.
Polycarbonate, also known as PC, is a thermoplastic polycondensate. Common trade names are Lexan and Makrolon. It has excellent strength, toughness, dimensional stability, dielectric strength, flame retardancy, and impact resistance (highest among transparent rigid materials). It is, however, susceptible to stress cracking with aromatic solvents, and is difficult to machine. PC can be used to make optical lenses, windows, medical items, CD's, and power tool housings. It can also be used in truck cabs.
Additional Information
Other common Polycarbonate (PC) include Unfilled Molding and Extrusion Resins, High Viscosity PC, Unfilled Molding and Extrusion Resins, Low Viscosity PC, 10% Glass Fiber Reinforced PC, 30% Glass Fiber Reinforced PC, 20 - 30% Long Glass Fiber Reinforced PC, 40% Long Glass Fiber Reinforced PC, 50% Long Glass Fiber Reinforced PC, 35% Random Glass Mat PC, 20 - 30% Long Glass Fiber Reinforced Flame-Retardant Grade PC, Polyester Copolymer High Heat PC, Polycarbonate Copolymer High Heat PC, Polycarbonate / Polyester Blends, Impact Modified PC, 6% Stainless Steel Fiber Conductive PC, 10% Stainless Steel Fiber EMI Shielding (conductive) PC, 20% PAN Carbon Fiber EMI Shielding (conductive) PC, 40% PAN Carbon Fiber EMI Shielding (conductive) PC, 10-15% PTFE Lubricated PC, 30% PTFE Lubricated PC, 10-15% PTFE, 20% Fiber Reinforced Lubricated PC, and 2% Silicone, 30% Glass Fiber Reinforced Lubricated PC.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1043
Glossary: Materials: Polymers: Polyester: Wholly Aromatic (liquid Crystal): 30% Glass Reinforced: High HDT Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4147 Glossary: Materials: Polymers: Polyetherimide: 30% Carbon Fiber: EMI Shielding (conductive) Glossary: Materials: Alloys: Steel: Tool Steel: AISI H14 Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 1335 Glossary: Materials: Alloys: Copper Alloy: Wire: AWG-30 Glossary: Materials: Alloys: Steel: Tool Steel: AISI L2 Glossary: Materials: Polymers: Polyimide: Thermoplastic: 30% Carbon Fiber Reinforced Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C50500 Related Pages
eFunda Polymers: Properties of Polycarbonate {polycarbonate ...
eFunda Polymers: Properties of Polycarbonate {polycarbonate / polyester blends, impact modified}
eFunda Polymers: Properties of Polyurethane {thermoplastic, 30 ...
... 30% PAN carbon fiber, EMI shielding (conductive)} ... State: thermoplastic. Additives: 30% PAN carbon fiber. Application: EMI shielding (conductive) ...
eFunda Polymers: Properties of Polycarbonate {35% random glass mat}
eFunda Polymers: Properties of Polycarbonate {35% random glass mat}
eFunda Polymers: Properties of ABS {40% aluminum flake, EMI ...
... Polymers: Properties of ABS {40% aluminum flake, EMI shielding (conductive)} ... Additives: 40% aluminum flake. Application: EMI shielding (conductive) ...
eFunda Polymers: Properties of Polyamide {nylon (PA 612), 10% PTFE ...
... of Polyamide {nylon (PA 612), 10% PTFE, 30% PAN carbon fiber, lubricated} ... Additives: 10% PTFE, 30% PAN carbon fiber. Application: lubricated ...
eFunda: Glossary: Units: Linear Mass Density: Denier
eFunda Polymers: Listing of Polycarbonate (Lexan, Makrolon). Units » Linear Mass Density » Denier · Units » Linear Mass Density » Pound (mass) Per Foot ...
eFunda Polymers: Properties of ABS {ABS / PC, flame-retardant ...
eFunda Polymers: Properties of ABS {ABS / PC, flame-retardant grades, molding and extrusion}
eFunda Polymers: Properties of Polycarbonate {10% glass fiber ...
eFunda Polymers: Properties of Polycarbonate {10% glass fiber reinforced}
eFunda Polymers: Properties of Polyetherimide {30% carbon fiber ...
... Properties of Polyetherimide {30% carbon fiber, EMI shielding (conductive)} ... Additives: 30% carbon fiber. Application: EMI shielding (conductive) ...
eFunda Polymers: Listing of Polyphenylene Sulfide (Ryton)
Polyphenylene Sulfide, 40% PAN carbon fiber, EMI shielding (conductive). 19. Polyphenylene Sulfide, 30% PAN carbon fiber, 15% PTFE, EMI shielding ...
|
||||||||