Polycarbonate: 50% Long Glass Fiber Reinforced
Home |
Directory |
Career |
News |
Industrial
|
|
|
|
Glossary » Materials » Polymers » Polycarbonate » 50% Long Glass Fiber Reinforced
50% Long Glass Fiber Reinforced PC is a subcategory of Polycarbonate. The additative is added by weight during the manufacturing process. Its tensile strength ranges from 25100 to 26000 MPa at break. Its elongation at break ranges from 1.3 to 1.5 %. Its molding pressure ranges from 10 to 20 MPa.
Polycarbonate, also known as PC, is a thermoplastic polycondensate. Common trade names are Lexan and Makrolon. It has excellent strength, toughness, dimensional stability, dielectric strength, flame retardancy, and impact resistance (highest among transparent rigid materials). It is, however, susceptible to stress cracking with aromatic solvents, and is difficult to machine. PC can be used to make optical lenses, windows, medical items, CD's, and power tool housings. It can also be used in truck cabs.
Additional Information
Other common Polycarbonate (PC) include Unfilled Molding and Extrusion Resins, High Viscosity PC, Unfilled Molding and Extrusion Resins, Low Viscosity PC, 10% Glass Fiber Reinforced PC, 30% Glass Fiber Reinforced PC, 20 - 30% Long Glass Fiber Reinforced PC, 40% Long Glass Fiber Reinforced PC, 35% Random Glass Mat PC, 20 - 30% Long Glass Fiber Reinforced Flame-Retardant Grade PC, Polyester Copolymer High Heat PC, Polycarbonate Copolymer High Heat PC, Polycarbonate / Polyester Blends, Impact Modified PC, 6% Stainless Steel Fiber Conductive PC, 10% Stainless Steel Fiber EMI Shielding (conductive) PC, 20% PAN Carbon Fiber EMI Shielding (conductive) PC, 30% PAN Carbon Fiber EMI Shielding (conductive) PC, 40% PAN Carbon Fiber EMI Shielding (conductive) PC, 10-15% PTFE Lubricated PC, 30% PTFE Lubricated PC, 10-15% PTFE, 20% Fiber Reinforced Lubricated PC, and 2% Silicone, 30% Glass Fiber Reinforced Lubricated PC.
Related Glossary Pages
Glossary: Materials: Polymers: Polyphenylene Sulfide: 30% Glass Fiber Reinforced
Glossary: Materials: Alloys: Aluminum Alloy: Cast: A356.0 Glossary: Materials: Alloys: Magnesium Alloy: ASTM HM21A-T8 Glossary: Materials: Alloys: Copper Alloy: Wire: AWG-2/0 Glossary: Materials: Polymers: Polyphenylene Sulfide: Encapsulation Grades Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 7050 Glossary: Materials: Polymers: Polyphthalamide: 15% Glass Reinforced, V-0 Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C98800 Glossary: Materials: Alloys: Steel: Stainless Steel: E-Brite26-1 Glossary: Materials: Polymers: Ethylene Vinyl Alcohol: Ethylene / Vinyl Alcohol Related Pages
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 50% long ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 50% long glass fiber reinforced} ... State: nylon (PA 6). Additives: 50% long glass fiber reinforced ...
eFunda Polymers: Properties of Polycarbonate {10% glass fiber ...
eFunda Polymers: Properties of Polycarbonate {10% glass fiber reinforced}
eFunda Polymers: Listing of Polycarbonate (Lexan, Makrolon)
Polycarbonate, also known as PC, has been mass-produced since 1958. ... Polycarbonate, unfilled, molding and extrusion resins, high viscosity. ...
eFunda Polymers: Properties of Polycarbonate {copolymer ...
eFunda Polymers: Properties of Polycarbonate {copolymer, polycarbonate copolymer
eFunda Polymers: Properties of Polycarbonate {6% stainless steel ...
eFunda Polymers: Properties of Polycarbonate {6% stainless steel fiber, conductive}
eFunda Polymers: Properties of Polyester (thermoset) {50% glass ...
Additives: 50% glass fiber reinforced. Application: high strength SMC ... Hardness, 50 - 60, Barcol, D638. Izod Impact (J/cm of notch) ...
eFunda Polymers: Properties of Polycarbonate {20% PAN carbon fiber ...
eFunda Polymers: Properties of Polycarbonate {20% PAN carbon fiber, EMI shielding (conductive)}
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 50% glass ...
State: nylon (PA 6). Additives: 50% glass fiber reinforced ... Top of Page. Related Glossary. Units » Mass » Quarter (US, Long) ...
eFunda: Glossary: Units: Linear Mass Density: Denier
eFunda Polymers: Listing of Polycarbonate (Lexan, Makrolon). Units » Linear Mass Density » Denier · Units » Linear Mass Density » Pound (mass) Per Foot ...
eFunda Polymers: Properties of Polyamide {partially aromatic, 50 ...
... Polymers: Properties of Polyamide {partially aromatic, 50% glass fiber reinforced} ... State: partially aromatic. Additives: 50% glass fiber reinforced ...
|
||||||||