Polycarbonate: Unfilled: Molding and Extrusion Resins, High Viscosity
Home |
Directory |
Career |
News |
Industrial
|
|
|
|
Glossary » Materials » Polymers » Polycarbonate » Unfilled » Molding and Extrusion Resins, High Viscosity
Unfilled Molding and Extrusion Resins, High Viscosity PC is a subcategory of Polycarbonate. The additative is added during the manufacturing process. Its flexural modulus ranges from 330 to 340 MPa. Its tensile strength ranges from 9100 to 10500 MPa at break. Its flexural strength ranges from 12500 to 13500 MPa. Its compressive strength ranges from 10000 to 12500 MPa. Its Izod Impact strength ranges from 12 to 18 J/cm. Its elongation at break ranges from 110 to 120 %. Its hardness ranges from 70 to 75 Rockwell M. Its molding pressure ranges from 10 to 20 MPa.
Polycarbonate, also known as PC, is a thermoplastic polycondensate. Common trade names are Lexan and Makrolon. It has excellent strength, toughness, dimensional stability, dielectric strength, flame retardancy, and impact resistance (highest among transparent rigid materials). It is, however, susceptible to stress cracking with aromatic solvents, and is difficult to machine. PC can be used to make optical lenses, windows, medical items, CD's, and power tool housings. It can also be used in truck cabs.
Additional Information
Other common Polycarbonate (PC) include Unfilled Molding and Extrusion Resins, Low Viscosity PC, 10% Glass Fiber Reinforced PC, 30% Glass Fiber Reinforced PC, 20 - 30% Long Glass Fiber Reinforced PC, 40% Long Glass Fiber Reinforced PC, 50% Long Glass Fiber Reinforced PC, 35% Random Glass Mat PC, 20 - 30% Long Glass Fiber Reinforced Flame-Retardant Grade PC, Polyester Copolymer High Heat PC, Polycarbonate Copolymer High Heat PC, Polycarbonate / Polyester Blends, Impact Modified PC, 6% Stainless Steel Fiber Conductive PC, 10% Stainless Steel Fiber EMI Shielding (conductive) PC, 20% PAN Carbon Fiber EMI Shielding (conductive) PC, 30% PAN Carbon Fiber EMI Shielding (conductive) PC, 40% PAN Carbon Fiber EMI Shielding (conductive) PC, 10-15% PTFE Lubricated PC, 30% PTFE Lubricated PC, 10-15% PTFE, 20% Fiber Reinforced Lubricated PC, and 2% Silicone, 30% Glass Fiber Reinforced Lubricated PC.
Related Glossary Pages
Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C10200
Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A573 Grade 65 Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 303Se Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1042 Glossary: Materials: Polymers: Polyphenylene Oxide: High Glass Transition Temp: Alloy With Polystyrene Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C86400 Glossary: Materials: Polymers: Allyl Resin: DAP: Glass Filled: Molding Compound Glossary: Materials: Alloys: Aluminum Alloy: Cast: 359.0 Glossary: Materials: Polymers: Polyester: Poly(butylene-Terephthalate): 35% Random Glass Mat Glossary: Materials: Alloys: Magnesium Alloy: ASTM AM60A-F Related Pages
eFunda Polymers: Properties of Fluoroplastics {fluorinated ...
eFunda Polymers: Properties of Fluoroplastics {fluorinated ethylene propylene, unfilled} ... State: fluorinated ethylene propylene. Additives: unfilled ...
eFunda Polymers: Properties of Fluoroplastics {modified PE-TFE ...
eFunda Polymers: Properties of Fluoroplastics {modified PE-TFE, unfilled} ... State: modified PE-TFE. Additives: unfilled ...
eFunda Polymers: Properties of Polypropylene {homopolymer, unfilled}
eFunda Polymers: Properties of Polypropylene {homopolymer, unfilled}
eFunda Polymers: Properties of Sulfone polymers {poly(ethersulfone ...
eFunda Polymers: Properties of Sulfone polymers {poly(ethersulfone), unfilled} ... State: poly(ethersulfone). Additives: unfilled ...
eFunda: Convert parsec to other Length units
Symbol: pc. Category: Length. SI Equivalent: 3.08568×1016 m ... Convert pc. 95 conversions, showing those commonly used | Show all ...
eFunda: Listing of Common Polymers (Plastics) in Chronological Order
It is susceptible to stress cracking with aromatic solvents, and is difficult to machine. -, Trade Name: Lexan, Makrolon. ...
eFunda Polymers: Properties of Polyamide {aromatic, unfilled ...
eFunda Polymers: Properties of Polyamide {aromatic, unfilled, aramid molded parts}
eFunda Polymers: Properties of Polypropylene {copolymer, unfilled}
eFunda Polymers: Properties of Polypropylene {copolymer, unfilled}
eFunda Polymers: Properties of Polycarbonate {copolymer ...
eFunda Polymers: Properties of Polycarbonate {copolymer, polycarbonate copolymer
eFunda Polymers: Properties of Polycarbonate {polycarbonate ...
eFunda Polymers: Properties of Polycarbonate {polycarbonate / polyester blends, impact modified}
|
||||||||