Glass Fiber Reinforced SMC Polyester is a subcategory of Polyester. The additative is added during the manufacturing process. Its elastic modulus ranges from 1400 to 2500 MPa. Its flexural modulus ranges from 1000 to 2200 MPa. Its tensile strength ranges from 7000 to 25000 MPa at break. Its flexural strength ranges from 10000 to 36000 MPa. Its compressive strength ranges from 15000 to 30000 MPa. Its Izod Impact strength ranges from 7 to 22 J/cm. Its hardness ranges from 50 to 70 . Its specific gravity ranges from 1.65 to 2.6. Its coefficient of thermal expansion ranges from 13.5 to 20 x 10-6/°C. Its molding pressure ranges from 0.3 to 2 MPa.
Polyester is a thermoplastic or thermoset polycondensate. Common trade names are Valox and Celanex. It has excellent dimensional stability, high dielectric strength, and good toughness. It has moderate chemical resistance, low resistance to strong acids and bases, and is notch sensitive. However, it is not recommended for outdoor use or in hot water. Polyester is very popular in making clothing and handles.
Additional Information
Other common Polyester include Rigid Polyester, Flexible Polyester, Glass Fiber Reinforced High Polyester, Glass Fiber Reinforced, Unidirectional Glass Polyester, Glass Fiber Reinforced, Preformed Chopped Roving Polyester, Glass Fiber Reinforced, Premix Chopped Glass Polyester, Glass Fiber Reinforced, Woven Cloth Polyester, Glass Fiber Reinforced SMC, BMC Low Density Polyester, Glass Fiber Reinforced SMC Low Pressure Polyester, Glass Fiber Reinforced SMC Low Shrink Polyester, Glass Fiber Reinforced BMC, TMC Polyester, EMI Shielding (conductive), SMC & TMC Polyester, EMI Shielding (conductive), BMC Polyester, and 50% Glass Fiber Reinforced High Strength SMC Polyester.
Related Glossary Pages
Glossary: Materials: Polymers: Melamine Formaldehyde: Cellulose Filled
Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 6201 Glossary: Materials: Alloys: Steel: Stainless Steel: Custom455TM Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C19200 Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A517 Grade B Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 310 Glossary: Materials: Polymers: Thermoplastic Elastomers: Silicone / Polyolefin: Pseudo-Interpenetrating Networks Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A441 Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 1335 Glossary: Materials: Polymers: Melamine Formaldehyde: Glass Fiber Reinforced Related Pages
eFunda Polymers: Properties of Polyamide {partially aromatic, 35 ...
... Properties of Polyamide {partially aromatic, 35% glass fiber reinforced, impact modified} ... Additives: 35% glass fiber reinforced, impact modified ...
eFunda Polymers: Properties of Polycarbonate {10% glass fiber ...
eFunda Polymers: Properties of Polycarbonate {10% glass fiber reinforced} ... Additives: 10% glass fiber reinforced. Material Properties ...
eFunda Polymers: Properties of Polyamide {partially aromatic, 60 ...
... Polymers: Properties of Polyamide {partially aromatic, 60% glass fiber reinforced} ... State: partially aromatic. Additives: 60% glass fiber reinforced ...
eFunda: Overview of Polymers (Plastics)
Introduction to polymers, their molecular structures and major grouping methods.
eFunda Polymers: Properties of Thermoplastic elastomers {silicone ...
... elastomers {silicone / polyester, psuedo-interpenetrating networks} ... State: silicone / polyester. Application: psuedo-interpenetrating networks ...
eFunda Polymers: Listing of Polyester (Valox, Celanex)
Polyester / alkyd, thermoset, alkyd, mineral filled, molding compounds, ... Polyester / alkyd, thermoset, vinyl ester, glass fiber reinforced, BMC. ...
eFunda: Comparisons between Polymers (Plastics) and Metals and ...
CRYSTALLINE POLYMERS: e.g., PPS, PBT (Valox), Polypropylene (PP), have. -, a sharply-defined melting point,. -, high shrinkage after molding, ...
eFunda Polymers: Properties of Polyurethane {thermoplastic, 30 ...
... Properties of Polyurethane {thermoplastic, 30% long glass fiber reinforced} ... State: thermoplastic. Additives: 30% long glass fiber reinforced ...
eFunda Polymers: Properties of Polyester / alkyd, thermoset {alkyd ...
eFunda Polymers: Properties of Polyester / alkyd, thermoset {alkyd, mineral filled, molding compounds, granular and putty}
eFunda Polymers: Properties of Polycarbonate {20 - 30% long glass ...
eFunda Polymers: Properties of Polycarbonate {20 - 30% long glass fiber reinforced} ... Additives: 20 - 30% long glass fiber reinforced ...
|
||||||||