Polyester: Glass Fiber Reinforced, Preformed Chopped Roving
Home |
Directory |
Career |
News |
Industrial
|
|
|
|
Glossary » Materials » Polymers » Polyester » Glass Fiber Reinforced, Preformed Chopped Roving
Glass Fiber Reinforced, Preformed Chopped Roving Polyester is a subcategory of Polyester. The additative is added during the manufacturing process. Its elastic modulus ranges from 800 to 2000 MPa. Its flexural modulus ranges from 1000 to 3000 MPa. Its tensile strength ranges from 15000 to 30000 MPa at break. Its flexural strength ranges from 10000 to 40000 MPa. Its compressive strength ranges from 15000 to 30000 MPa. Its Izod Impact strength ranges from 2 to 20 J/cm. Its elongation at break ranges from 1 to 5 %. Its hardness ranges from 50 to 80 . Its specific gravity ranges from 1.35 to 2.3. Its coefficient of thermal expansion ranges from 20 to 50 x 10-6/°C. Its molding pressure ranges from 0.25 to 2 MPa.
Polyester is a thermoplastic or thermoset polycondensate. Common trade names are Valox and Celanex. It has excellent dimensional stability, high dielectric strength, and good toughness. It has moderate chemical resistance, low resistance to strong acids and bases, and is notch sensitive. However, it is not recommended for outdoor use or in hot water. Polyester is very popular in making clothing and handles.
Additional Information
Other common Polyester include Rigid Polyester, Flexible Polyester, Glass Fiber Reinforced High Polyester, Glass Fiber Reinforced, Unidirectional Glass Polyester, Glass Fiber Reinforced, Premix Chopped Glass Polyester, Glass Fiber Reinforced, Woven Cloth Polyester, Glass Fiber Reinforced SMC Polyester, Glass Fiber Reinforced SMC, BMC Low Density Polyester, Glass Fiber Reinforced SMC Low Pressure Polyester, Glass Fiber Reinforced SMC Low Shrink Polyester, Glass Fiber Reinforced BMC, TMC Polyester, EMI Shielding (conductive), SMC & TMC Polyester, EMI Shielding (conductive), BMC Polyester, and 50% Glass Fiber Reinforced High Strength SMC Polyester.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 3140
Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C95700 Glossary: Materials: Polymers: Polypropylene: Copolymer: Unfilled Glossary: Materials: Polymers: Silicone: Copolymer: Silicone / Nylon 12: Psuedo-Interpenetrating Networks Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A538 Grade A Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A202 Grade A Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 302B Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1045 Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C94900 Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 86B45H Related Pages
eFunda: Listing of Common Polymers (Plastics)
eFunda: Listing of Common Polymers (Plastics) ... Cellulosic, Thermoplastic modified natural polymer substance. Epoxy, Thermoset polyadduct. ...
eFunda Polymers: Properties of Epoxy {bisphenol, glass fiber ...
eFunda Polymers: Properties of Epoxy {bisphenol, glass fiber reinforced, ... Additives: glass fiber reinforced. Application: molding compounds ...
eFunda Polymers: Listing of Liquid Crystal Polymer (Vectra, Xydar)
Liquid Crystal Polymer, also known as LCP, has been mass-produced since 1980. ... Liquid Crystal Polymer, glass fiber reinforced, used for SMT. ...
eFunda Polymers: Properties of Polyester (thermoset) {EMI ...
eFunda Polymers: Properties of Polyester (thermoset) {EMI shielding (conductive)
eFunda: Polymer (Plastic) Supplier Contact Information
Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219. Phone: 718-851-8111 ... Bamberger Polymers, Inc. 2 Jericho Plaza. Jericho, NY 11753 ...
eFunda Polymers: Properties of Polycarbonate {20 - 30% long glass ...
eFunda Polymers: Properties of Polycarbonate {20 - 30% long glass fiber reinforced} ... Additives: 20 - 30% long glass fiber reinforced ...
eFunda Polymers: Properties of Polyester / alkyd, thermoset {alkyd ...
eFunda Polymers: Properties of Polyester / alkyd, thermoset {alkyd, mineral filled, molding compounds, granular and putty}
eFunda Polymers: Properties of Polycarbonate {copolymer, polyester ...
eFunda Polymers: Properties of Polycarbonate {copolymer, polyester copolymer, high heat}
eFunda: Listing of Common Polymers (Plastics) in Chronological Order
... low resistance to strong acids and bases, is notch sensitive, and is not recommended for outdoor use or in hot water. -, Trade Name: Valox, Celanex. ...
eFunda Polymers: Properties of Polyamide {partially aromatic, 35 ...
... Properties of Polyamide {partially aromatic, 35% glass fiber reinforced, impact modified} ... Additives: 35% glass fiber reinforced, impact modified ...
|
||||||||