Polyester: Poly(butylene-Terephthalate): 30% Long Glass Fiber Reinforced
Home |
Directory |
Career |
News |
Industrial
|
|
|
|
Glossary » Materials » Polymers » Polyester » 30% Long Glass Fiber Reinforced
30% Long Glass Fiber Reinforced Polyester is a subcategory of Polyester. The additative is added by weight during the manufacturing process. Its molding pressure ranges from 10 to 20 MPa.
Polyester is a thermoplastic or thermoset polycondensate. Common trade names are Valox and Celanex. poly(butylene-terephthalate) It has excellent dimensional stability, high dielectric strength, and good toughness. It has moderate chemical resistance, low resistance to strong acids and bases, and is notch sensitive. However, it is not recommended for outdoor use or in hot water. Polyester is very popular in making clothing and handles.
Additional Information
Other common Polyester include Unfilled Polyester, 30% Glass Fiber Reinforced Polyester, 40% Long Glass Fiber Reinforced Polyester, 50% Long Glass Fiber Reinforced Polyester, 60% Long Glass Fiber Reinforced Polyester, 25% Random Glass Mat Polyester, 35% Random Glass Mat Polyester, 40-50% Glass Fiber and Mineral Reinforced Polyester, 35% Glass Fiber and Mica Reinforced Polyester, Impact Modified Polyester, 50% Glass Fiber Reinforced Polyester, 7 - 15% Glass Fiber Reinforced Flame-Retardant Grade Polyester, 35% Glass Fiber Reinforced Flame-Retardant Grade Polyester, 30% Carbon Fiber EMI Shielding (conductive) Polyester, Unfilled Polyester, 7.0 - 30% Glass Fiber Reinforced Polyester, Unreinforced Flame-Retardant Polyester, 15% Glass Fiber Reinforced Polyester, 30% Glass Fiber Reinforced Polyester, 40% Glass Fiber Reinforced Polyester, 27 - 30% Glass Fiber and Mineral Reinforced Polyester, 40% Glass Fiber and Mineral Reinforced Polyester, 20% Glass Flame-Retardant Polyester, 30% Glass Flame-Retardant Polyester, 40% Glass Flame-Retardant Polyester, 15% Glass Fiber Reinforced Polyester, 20% Glass Fibre Reinforced Polyester, 30% Glass Fiber Reinforced Polyester, Unfilled Polyester, Unfilled Polyester, 15% Glass Fiber Reinforced Polyester, 30% Glass Fiber Reinforced Polyester, 40 - 45% Glass Fiber Reinforced Polyester, 35% Glass, Super Toughened Polyester, 15% Glass Easy Processing Polyester, 30% Glass Flame-Retardant, V-0 1/32 Polyester, 15% Glass Flame-Retardant, V-0 1/32 Polyester, 15-20% Glass Flame-Retardant Polyester, 30% Glass Flame-Retardant Polyester, 40% Glass Flame-Retardant Polyester, 35 - 45% Glass Fiber and Mica Reinforced Polyester, 30% Long Glass Fiber Reinforced Polyester, 40% Long Glass Fiber Reinforced Polyester, 50% Long Glass Fiber Reinforced Polyester, 60% Long Glass Fiber Reinforced Polyester, 30% PAN Carbon Fiber EMI Shielding (conductive) Polyester, Recycled Content, 30% Glass Fiber Polyester, Recycled Content, 45% Glass Fiber Polyester, Recycled Content, 35% Glass/mineral Reinforced Polyester, Unfilled PETG Polyester, Unfilled Copolyester Polyester, P / PC Blend High Impact Polyester, P / PC Blend, 30% Glass Fiber Reinforced Polyester, P / PC Blend Flame-Retardant Polyester, Unfilled Medium Melting Point Polyester, Unfilled High Melting Point Polyester, 30% Carbon Fiber Reinforced Polyester, 40% Glass Fiber Filled Polyester, 40% Glass Plus 10% Mineral Filled Polyester, 30 - 50% Mineral Filled Polyester, 30% Glass Fiber Reinforced Polyester, 30% Glass Reinforced High HDT Polyester, and Unfilled Platable Grade Polyester.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4615
Glossary: Materials: Polymers: Polyurethane: Thermoset: Casting Resin, Liquid Glossary: Materials: Polymers: Fluoroplastics: PE-CTFE Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 5130H Glossary: Materials: Polymers: Polyamide: Nylon (PA 66): 25-30% Mineral Filled, Modified High-Impact Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A611 Grade E Glossary: Materials: Polymers: Epoxy: Bisphenol: Glass Fiber Reinforced: Molding Compounds Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1049 Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A737 Grade B Glossary: Materials: Polymers: Polyamide: Nylon (PA 66): 5% Silicone: Lubricated Related Pages
eFunda: Polymer (Plastic) Supplier Contact Information
American Polymers, Inc. 53 Millbrook St. P.O. Box 60398. Worcester, MA 01606 ... Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219 ...
eFunda Polymers: Properties of ABS {30% glass fiber reinforced ...
eFunda Polymers: Properties of ABS {30% glass fiber reinforced, injection molding grade}
eFunda Polymers: Properties of Polyphenylene Sulfide {30% long ...
Trade Publications. Reinforced Plastics · What Is ISO 14001 · Medical Device ... Additives: 30% long glass fiber reinforced. Material Properties ...
eFunda Polymers: Properties of Polyamide {nylon (PA 610), 30 ...
Trade Publications. Reinforced Plastics · Design-2-Part · Chemical Processing ... Additives: 30% glass fiber reinforced. Application: flame-retardant grade ...
eFunda: Polymer (Plastic) Supplier Contact Information
Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219. Phone: 718-851-8111 ... Bamberger Polymers, Inc. 2 Jericho Plaza. Jericho, NY 11753 ...
eFunda: Properties of Piezo Material Lead Zirconate Titanate (PZT-5A)
eFunda: Properties of Piezo Material Lead Zirconate Titanate (PZT-5A)
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 30% glass ...
... Polymers: Properties of Polyamide {nylon (PA 6), 30% glass fiber reinforced, impact modified} ... Additives: 30% glass fiber reinforced, impact modified ...
eFunda Polymers: Properties of Thermoplastic elastomers {silicone ...
... elastomers {silicone / polyester, psuedo-interpenetrating networks} ... State: silicone / polyester. Application: psuedo-interpenetrating networks ...
Properties of Common Solid Materials
Further information on a specific material can be obtained by clicking the name of that particular material in the following table. ...
eFunda Polymers: Properties of Polyamide {nylon (PA 610), 30-40 ...
Reinforced Plastics · appliance DESIGN · Test & Measurement · Business Aviation ... State: nylon (PA 610). Additives: 30-40% long glass fiber reinforced ...
|
||||||||