Polyester: Poly(cyclohexylene-Methylene-Terephthalate): 20% Glass Fibre Reinforced
Home |
Directory |
Career |
News |
Industrial
|
|
|
|
Glossary » Materials » Polymers » Polyester » 20% Glass Fibre Reinforced
20% Glass Fibre Reinforced Polyester is a subcategory of Polyester. The additative is added by weight during the manufacturing process. Its molding pressure ranges from 8 to 16 MPa.
Polyester is a thermoplastic or thermoset polycondensate. Common trade names are Valox and Celanex. poly(cyclohexylene-methylene-terephthalate) It has excellent dimensional stability, high dielectric strength, and good toughness. It has moderate chemical resistance, low resistance to strong acids and bases, and is notch sensitive. However, it is not recommended for outdoor use or in hot water. Polyester is very popular in making clothing and handles.
Additional Information
Other common Polyester include Unfilled Polyester, 30% Glass Fiber Reinforced Polyester, 30% Long Glass Fiber Reinforced Polyester, 40% Long Glass Fiber Reinforced Polyester, 50% Long Glass Fiber Reinforced Polyester, 60% Long Glass Fiber Reinforced Polyester, 25% Random Glass Mat Polyester, 35% Random Glass Mat Polyester, 40-50% Glass Fiber and Mineral Reinforced Polyester, 35% Glass Fiber and Mica Reinforced Polyester, Impact Modified Polyester, 50% Glass Fiber Reinforced Polyester, 7 - 15% Glass Fiber Reinforced Flame-Retardant Grade Polyester, 35% Glass Fiber Reinforced Flame-Retardant Grade Polyester, 30% Carbon Fiber EMI Shielding (conductive) Polyester, Unfilled Polyester, 7.0 - 30% Glass Fiber Reinforced Polyester, Unreinforced Flame-Retardant Polyester, 15% Glass Fiber Reinforced Polyester, 30% Glass Fiber Reinforced Polyester, 40% Glass Fiber Reinforced Polyester, 27 - 30% Glass Fiber and Mineral Reinforced Polyester, 40% Glass Fiber and Mineral Reinforced Polyester, 20% Glass Flame-Retardant Polyester, 30% Glass Flame-Retardant Polyester, 40% Glass Flame-Retardant Polyester, 15% Glass Fiber Reinforced Polyester, 30% Glass Fiber Reinforced Polyester, Unfilled Polyester, Unfilled Polyester, 15% Glass Fiber Reinforced Polyester, 30% Glass Fiber Reinforced Polyester, 40 - 45% Glass Fiber Reinforced Polyester, 35% Glass, Super Toughened Polyester, 15% Glass Easy Processing Polyester, 30% Glass Flame-Retardant, V-0 1/32 Polyester, 15% Glass Flame-Retardant, V-0 1/32 Polyester, 15-20% Glass Flame-Retardant Polyester, 30% Glass Flame-Retardant Polyester, 40% Glass Flame-Retardant Polyester, 35 - 45% Glass Fiber and Mica Reinforced Polyester, 30% Long Glass Fiber Reinforced Polyester, 40% Long Glass Fiber Reinforced Polyester, 50% Long Glass Fiber Reinforced Polyester, 60% Long Glass Fiber Reinforced Polyester, 30% PAN Carbon Fiber EMI Shielding (conductive) Polyester, Recycled Content, 30% Glass Fiber Polyester, Recycled Content, 45% Glass Fiber Polyester, Recycled Content, 35% Glass/mineral Reinforced Polyester, Unfilled PETG Polyester, Unfilled Copolyester Polyester, P / PC Blend High Impact Polyester, P / PC Blend, 30% Glass Fiber Reinforced Polyester, P / PC Blend Flame-Retardant Polyester, Unfilled Medium Melting Point Polyester, Unfilled High Melting Point Polyester, 30% Carbon Fiber Reinforced Polyester, 40% Glass Fiber Filled Polyester, 40% Glass Plus 10% Mineral Filled Polyester, 30 - 50% Mineral Filled Polyester, 30% Glass Fiber Reinforced Polyester, 30% Glass Reinforced High HDT Polyester, and Unfilled Platable Grade Polyester.
Related Glossary Pages
Glossary: Materials: Polymers: Acrylonitrile-Butadiene-Styrene: 20% Graphite Fiber: EMI Shielding (conductive)
Glossary: Materials: Polymers: Acrylonitrile-Butadiene-Styrene: ABS / PC: Injection Molding and Extrusion Glossary: Materials: Polymers: Liquid Crystal Polymer: 15% Glass Fiber Reinforced Glossary: Materials: Polymers: Polyaryletherketone: Poly(etherether-Ketone): 30% Glass Fiber Reinforced Glossary: Materials: Polymers: Polyvinylchloride: Copolymer: PVC / Acrylic Blends: Molding and Extrusion Compounds Glossary: Materials: Polymers: Phenol-Formaldehyde Plastic: Phenol-Formaldehyde: High Strength Glass Fiber Reinforced: Molding Compounds Glossary: Materials: Polymers: Polyamide: Nylon (PA 6): 33% Glass Fiber Reinforced, Toughened Glossary: Materials: Alloys: Steel: Stainless Steel: 18-2FM Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C22000 Glossary: Materials: Polymers: Silicone: Mineral And/or Glass Filled: Molding and Encapsulating Compounds Related Pages
eFunda Polymers: Properties of Polyester (thermoplastic) {poly ...
eFunda Polymers: Properties of Polyester (thermoplastic) {poly(butylene-
eFunda Polymers: Properties of Thermoplastic elastomers {silicone ...
... elastomers {silicone / polyester, psuedo-interpenetrating networks} ... State: silicone / polyester. Application: psuedo-interpenetrating networks ...
eFunda Polymers: Properties of Sulfone polymers {polysulfone, 20 ...
eFunda Polymers: Properties of Sulfone polymers {polysulfone, 20% glass fiber reinforced} ... State: polysulfone. Additives: 20% glass fiber reinforced ...
eFunda: Estimanation of Lamina Material Constants
Calculates the equivalent material constants for a fiber reinforced composite lamina.
Properties of Common Solid Materials
Further information on a specific material can be obtained by clicking the name of that particular material in the following table. ...
eFunda: Properties of Piezo Material Lead Zirconate Titanate (PZT-5A)
eFunda: Properties of Piezo Material Lead Zirconate Titanate (PZT-5A)
eFunda: Polymer (Plastic) Supplier Contact Information
Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219. Phone: 718-851-8111 ... Bamberger Polymers, Inc. 2 Jericho Plaza. Jericho, NY 11753 ...
eFunda: Glossary of Polymers (Plastics)
Common terms used in material science of polymers.
eFunda: Engineering Materials
Home page for properties of materials such as elements, alloys, polymers, and piezo ceramics.
eFunda Polymers: Listing of Polycarbonate (Lexan, Makrolon)
Polycarbonate, 20 - 30% long glass fiber reinforced, flame-retardant grade. 10. Polycarbonate, copolymer, polyester copolymer, high heat. ...
|
||||||||