Polyester: Poly(cyclohexylene-Methylene-Terephthalate): 40% Glass
Home |
Directory |
Career |
News |
Industrial
|
|
|
|
Glossary » Materials » Polymers » Polyester » Poly(cyclohexylene-Methylene-Terephthalate) » 40% Glass » Flame-Retardant
40% Glass Flame-Retardant Polyester is a subcategory of Polyester. The additative is added by weight during the manufacturing process.
Polyester is a thermoplastic or thermoset polycondensate. Common trade names are Valox and Celanex. poly(cyclohexylene-methylene-terephthalate) It has excellent dimensional stability, high dielectric strength, and good toughness. It has moderate chemical resistance, low resistance to strong acids and bases, and is notch sensitive. However, it is not recommended for outdoor use or in hot water. Polyester is very popular in making clothing and handles.
Additional Information
Other common Polyester include Unfilled Polyester, 30% Glass Fiber Reinforced Polyester, 30% Long Glass Fiber Reinforced Polyester, 40% Long Glass Fiber Reinforced Polyester, 50% Long Glass Fiber Reinforced Polyester, 60% Long Glass Fiber Reinforced Polyester, 25% Random Glass Mat Polyester, 35% Random Glass Mat Polyester, 40-50% Glass Fiber and Mineral Reinforced Polyester, 35% Glass Fiber and Mica Reinforced Polyester, Impact Modified Polyester, 50% Glass Fiber Reinforced Polyester, 7 - 15% Glass Fiber Reinforced Flame-Retardant Grade Polyester, 35% Glass Fiber Reinforced Flame-Retardant Grade Polyester, 30% Carbon Fiber EMI Shielding (conductive) Polyester, Unfilled Polyester, 7.0 - 30% Glass Fiber Reinforced Polyester, Unreinforced Flame-Retardant Polyester, 15% Glass Fiber Reinforced Polyester, 30% Glass Fiber Reinforced Polyester, 40% Glass Fiber Reinforced Polyester, 27 - 30% Glass Fiber and Mineral Reinforced Polyester, 40% Glass Fiber and Mineral Reinforced Polyester, 20% Glass Flame-Retardant Polyester, 30% Glass Flame-Retardant Polyester, 15% Glass Fiber Reinforced Polyester, 20% Glass Fibre Reinforced Polyester, 30% Glass Fiber Reinforced Polyester, Unfilled Polyester, Unfilled Polyester, 15% Glass Fiber Reinforced Polyester, 30% Glass Fiber Reinforced Polyester, 40 - 45% Glass Fiber Reinforced Polyester, 35% Glass, Super Toughened Polyester, 15% Glass Easy Processing Polyester, 30% Glass Flame-Retardant, V-0 1/32 Polyester, 15% Glass Flame-Retardant, V-0 1/32 Polyester, 15-20% Glass Flame-Retardant Polyester, 30% Glass Flame-Retardant Polyester, 40% Glass Flame-Retardant Polyester, 35 - 45% Glass Fiber and Mica Reinforced Polyester, 30% Long Glass Fiber Reinforced Polyester, 40% Long Glass Fiber Reinforced Polyester, 50% Long Glass Fiber Reinforced Polyester, 60% Long Glass Fiber Reinforced Polyester, 30% PAN Carbon Fiber EMI Shielding (conductive) Polyester, Recycled Content, 30% Glass Fiber Polyester, Recycled Content, 45% Glass Fiber Polyester, Recycled Content, 35% Glass/mineral Reinforced Polyester, Unfilled PETG Polyester, Unfilled Copolyester Polyester, P / PC Blend High Impact Polyester, P / PC Blend, 30% Glass Fiber Reinforced Polyester, P / PC Blend Flame-Retardant Polyester, Unfilled Medium Melting Point Polyester, Unfilled High Melting Point Polyester, 30% Carbon Fiber Reinforced Polyester, 40% Glass Fiber Filled Polyester, 40% Glass Plus 10% Mineral Filled Polyester, 30 - 50% Mineral Filled Polyester, 30% Glass Fiber Reinforced Polyester, 30% Glass Reinforced High HDT Polyester, and Unfilled Platable Grade Polyester.
Related Glossary Pages
Glossary: Materials: Polymers: Polyamide: Nylon (PA 66): 40% Aluminum Flake: EMI Shielding (conductive)
Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A724 Grade A Glossary: Materials: Polymers: Polyamide: Aromatic, Amorphous Transparent Copolymer Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4028H Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C62300 Glossary: Materials: Alloys: Titanium Alloy: Wrought: Ti-8Al-1Mo-1V Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C10200 Glossary: Materials: Alloys: Aluminum Alloy: Wrought: AA 1100 Glossary: Materials: Alloys: Copper Alloy: Wire: AWG-38 Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C81700 Related Pages
eFunda Polymers: Properties of Acetal {40% long glass fiber ...
eFunda Polymers: Properties of Acetal {40% long glass fiber reinforced}
eFunda: Polymer (Plastic) Supplier Contact Information
Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219. Phone: 718-851-8111 ... Bamberger Polymers, Inc. 2 Jericho Plaza. Jericho, NY 11753 ...
eFunda Polymers: Properties of Thermoplastic elastomers {polyester}
eFunda Polymers: Properties of Thermoplastic elastomers {polyester}
eFunda Polymers: Properties of Sulfone polymers {polysulfone ...
... of Sulfone polymers {polysulfone, injection molding, flame-retardant, extrusion} ... Application: injection molding, flame-retardant, extrusion ...
eFunda Polymers: Properties of Polycarbonate {20 - 30% long glass ...
eFunda Polymers: Properties of Polycarbonate {20 - 30% long glass fiber reinforced, flame-retardant grade}
eFunda: Overview of Polymers (Plastics)
Introduction to polymers, their molecular structures and major grouping methods.
eFunda: Property Dependancies of Polymers (Plastics)
Flame-retardants are added to minimize the chance of a material igniting. For a material to be considered flame-retardant, it needs to meet the UL ...
eFunda Polymers: Properties of Polyphenylene Sulfide {40% glass ...
eFunda Polymers: Properties of Polyphenylene Sulfide {40% glass fiber reinforced
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 40% long ...
eFunda Polymers: Properties of Polyamide {nylon (PA 6), 40% long glass fiber reinforced} ... State: nylon (PA 6). Additives: 40% long glass fiber reinforced ...
eFunda Polymers: Properties of Polyamide {partially aromatic, 40 ...
eFunda Polymers: Properties of Polyamide {partially aromatic, 40% glass fiber ... State: partially aromatic. Additives: 40% glass fiber reinforced ...
|
||||||||