Polyester: Poly(ethylene-Terephthalate): 15% Glass Fiber Reinforced
Home |
Directory |
Career |
News |
Industrial
|
|
|
|
Glossary » Materials » Polymers » Polyester » 15% Glass Fiber Reinforced
15% Glass Fiber Reinforced Polyester is a subcategory of Polyester. The additative is added by weight during the manufacturing process.
Polyester is a thermoplastic or thermoset polycondensate. Common trade names are Valox and Celanex. poly(ethylene-terephthalate) It has excellent dimensional stability, high dielectric strength, and good toughness. It has moderate chemical resistance, low resistance to strong acids and bases, and is notch sensitive. However, it is not recommended for outdoor use or in hot water. Polyester is very popular in making clothing and handles.
Additional Information
Other common Polyester include Unfilled Polyester, 30% Glass Fiber Reinforced Polyester, 30% Long Glass Fiber Reinforced Polyester, 40% Long Glass Fiber Reinforced Polyester, 50% Long Glass Fiber Reinforced Polyester, 60% Long Glass Fiber Reinforced Polyester, 25% Random Glass Mat Polyester, 35% Random Glass Mat Polyester, 40-50% Glass Fiber and Mineral Reinforced Polyester, 35% Glass Fiber and Mica Reinforced Polyester, Impact Modified Polyester, 50% Glass Fiber Reinforced Polyester, 7 - 15% Glass Fiber Reinforced Flame-Retardant Grade Polyester, 35% Glass Fiber Reinforced Flame-Retardant Grade Polyester, 30% Carbon Fiber EMI Shielding (conductive) Polyester, Unfilled Polyester, 7.0 - 30% Glass Fiber Reinforced Polyester, Unreinforced Flame-Retardant Polyester, 15% Glass Fiber Reinforced Polyester, 30% Glass Fiber Reinforced Polyester, 40% Glass Fiber Reinforced Polyester, 27 - 30% Glass Fiber and Mineral Reinforced Polyester, 40% Glass Fiber and Mineral Reinforced Polyester, 20% Glass Flame-Retardant Polyester, 30% Glass Flame-Retardant Polyester, 40% Glass Flame-Retardant Polyester, 15% Glass Fiber Reinforced Polyester, 20% Glass Fibre Reinforced Polyester, 30% Glass Fiber Reinforced Polyester, Unfilled Polyester, Unfilled Polyester, 30% Glass Fiber Reinforced Polyester, 40 - 45% Glass Fiber Reinforced Polyester, 35% Glass, Super Toughened Polyester, 15% Glass Easy Processing Polyester, 30% Glass Flame-Retardant, V-0 1/32 Polyester, 15% Glass Flame-Retardant, V-0 1/32 Polyester, 15-20% Glass Flame-Retardant Polyester, 30% Glass Flame-Retardant Polyester, 40% Glass Flame-Retardant Polyester, 35 - 45% Glass Fiber and Mica Reinforced Polyester, 30% Long Glass Fiber Reinforced Polyester, 40% Long Glass Fiber Reinforced Polyester, 50% Long Glass Fiber Reinforced Polyester, 60% Long Glass Fiber Reinforced Polyester, 30% PAN Carbon Fiber EMI Shielding (conductive) Polyester, Recycled Content, 30% Glass Fiber Polyester, Recycled Content, 45% Glass Fiber Polyester, Recycled Content, 35% Glass/mineral Reinforced Polyester, Unfilled PETG Polyester, Unfilled Copolyester Polyester, P / PC Blend High Impact Polyester, P / PC Blend, 30% Glass Fiber Reinforced Polyester, P / PC Blend Flame-Retardant Polyester, Unfilled Medium Melting Point Polyester, Unfilled High Melting Point Polyester, 30% Carbon Fiber Reinforced Polyester, 40% Glass Fiber Filled Polyester, 40% Glass Plus 10% Mineral Filled Polyester, 30 - 50% Mineral Filled Polyester, 30% Glass Fiber Reinforced Polyester, 30% Glass Reinforced High HDT Polyester, and Unfilled Platable Grade Polyester.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 8720H
Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 304H Glossary: Materials: Polymers: Polyester: P / PC Blend, 30% Glass Fiber Reinforced Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A387 Grade 9 Glossary: Materials: Polymers: Thermoplastic Elastomers: Silicone / Polyurethane: Aromatic and Aliphatic Polyether and Polyester Urethane, Unfilled: Pseudo-Interpenetrating Networks Glossary: Materials: Alloys: Titanium Alloy: Wrought: Ti-3Al-8V-6Cr-4Mo-4Zr Glossary: Materials: Polymers: Polyaryletherketone: Poly(etherether-Ketone): 30% Glass Fiber Reinforced Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1075 Glossary: Materials: Polymers: Polyamide: Nylon (PA 6): 50% Glass Fiber Reinforced Glossary: Materials: Alloys: Copper Alloy: Cast: UNS C81500 Related Pages
eFunda Polymers: Properties of Polyamide {nylon (PA 612), 15% PTFE ...
... {nylon (PA 612), 15% PTFE, 30% glass fiber reinforced, lubricated} ... Additives: 15% PTFE, 30% glass fiber reinforced. Application: lubricated ...
Properties of Common Solid Materials
Further information on a specific material can be obtained by clicking the name of that particular material in the following table. ...
eFunda Polymers: Properties of Ketones {poly(arylether-ketone), 40 ...
State: poly(arylether-ketone). Additives: 40% glass fiber reinforced ... Melt Flow (gm/10 min), 15 - 25, D1238. Melting Temperature (ºC), 329 ...
eFunda Polymers: Properties of Polycarbonate {polycarbonate ...
eFunda Polymers: Properties of Polycarbonate {polycarbonate / polyester blends, ... Additives: polycarbonate / polyester blends, impact modified ...
eFunda: Listing of Common Polymers (Plastics) in Chronological Order
... low resistance to strong acids and bases, is notch sensitive, and is not recommended for outdoor use or in hot water. -, Trade Name: Valox, Celanex. ...
eFunda: Properties of Piezo Material Lead Zirconate Titanate (PZT-5A)
eFunda: Properties of Piezo Material Lead Zirconate Titanate (PZT-5A)
eFunda: Glossary of Polymers (Plastics)
Common terms used in material science of polymers.
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 15-33 ...
eFunda Polymers: Properties of Polyamide {nylon (PA 66), 15-33% glass fiber reinforced, toughened} ... Additives: 15-33% glass fiber reinforced, toughened ...
eFunda: Polymer (Plastic) Supplier Contact Information
Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219. Phone: 718-851-8111 ... Bamberger Polymers, Inc. 2 Jericho Plaza. Jericho, NY 11753 ...
eFunda: Piezo Material Data
Select specific piezoelectric material to view constitutive properties.
|
||||||||