Polyester: Poly(ethylene-Terephthalate): Recycled Content, 30% Glass Fiber
Home |
Directory |
Career |
News |
Industrial
|
|
|
|
Glossary » Materials » Polymers » Polyester » Recycled Content, 30% Glass Fiber
Recycled Content, 30% Glass Fiber Polyester is a subcategory of Polyester. The additative is added by weight during the manufacturing process.
Polyester is a thermoplastic or thermoset polycondensate. Common trade names are Valox and Celanex. poly(ethylene-terephthalate) It has excellent dimensional stability, high dielectric strength, and good toughness. It has moderate chemical resistance, low resistance to strong acids and bases, and is notch sensitive. However, it is not recommended for outdoor use or in hot water. Polyester is very popular in making clothing and handles.
Additional Information
Other common Polyester include Unfilled Polyester, 30% Glass Fiber Reinforced Polyester, 30% Long Glass Fiber Reinforced Polyester, 40% Long Glass Fiber Reinforced Polyester, 50% Long Glass Fiber Reinforced Polyester, 60% Long Glass Fiber Reinforced Polyester, 25% Random Glass Mat Polyester, 35% Random Glass Mat Polyester, 40-50% Glass Fiber and Mineral Reinforced Polyester, 35% Glass Fiber and Mica Reinforced Polyester, Impact Modified Polyester, 50% Glass Fiber Reinforced Polyester, 7 - 15% Glass Fiber Reinforced Flame-Retardant Grade Polyester, 35% Glass Fiber Reinforced Flame-Retardant Grade Polyester, 30% Carbon Fiber EMI Shielding (conductive) Polyester, Unfilled Polyester, 7.0 - 30% Glass Fiber Reinforced Polyester, Unreinforced Flame-Retardant Polyester, 15% Glass Fiber Reinforced Polyester, 30% Glass Fiber Reinforced Polyester, 40% Glass Fiber Reinforced Polyester, 27 - 30% Glass Fiber and Mineral Reinforced Polyester, 40% Glass Fiber and Mineral Reinforced Polyester, 20% Glass Flame-Retardant Polyester, 30% Glass Flame-Retardant Polyester, 40% Glass Flame-Retardant Polyester, 15% Glass Fiber Reinforced Polyester, 20% Glass Fibre Reinforced Polyester, 30% Glass Fiber Reinforced Polyester, Unfilled Polyester, Unfilled Polyester, 15% Glass Fiber Reinforced Polyester, 30% Glass Fiber Reinforced Polyester, 40 - 45% Glass Fiber Reinforced Polyester, 35% Glass, Super Toughened Polyester, 15% Glass Easy Processing Polyester, 30% Glass Flame-Retardant, V-0 1/32 Polyester, 15% Glass Flame-Retardant, V-0 1/32 Polyester, 15-20% Glass Flame-Retardant Polyester, 30% Glass Flame-Retardant Polyester, 40% Glass Flame-Retardant Polyester, 35 - 45% Glass Fiber and Mica Reinforced Polyester, 30% Long Glass Fiber Reinforced Polyester, 40% Long Glass Fiber Reinforced Polyester, 50% Long Glass Fiber Reinforced Polyester, 60% Long Glass Fiber Reinforced Polyester, 30% PAN Carbon Fiber EMI Shielding (conductive) Polyester, Recycled Content, 45% Glass Fiber Polyester, Recycled Content, 35% Glass/mineral Reinforced Polyester, Unfilled PETG Polyester, Unfilled Copolyester Polyester, P / PC Blend High Impact Polyester, P / PC Blend, 30% Glass Fiber Reinforced Polyester, P / PC Blend Flame-Retardant Polyester, Unfilled Medium Melting Point Polyester, Unfilled High Melting Point Polyester, 30% Carbon Fiber Reinforced Polyester, 40% Glass Fiber Filled Polyester, 40% Glass Plus 10% Mineral Filled Polyester, 30 - 50% Mineral Filled Polyester, 30% Glass Fiber Reinforced Polyester, 30% Glass Reinforced High HDT Polyester, and Unfilled Platable Grade Polyester.
Related Glossary Pages
Glossary: Materials: Polymers: Polyamide: Nylon (PA 46): 50% Glass and Mineral Filled
Glossary: Materials: Alloys: Steel: Stainless Steel: Monit Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 51B60H Glossary: Materials: Polymers: Polyamide: Nylon (PA 46): 50% Glass Reinforced Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A678 Grade B Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A517 Grade C Glossary: Materials: Polymers: Polyamide: Nylon (PA 66): 40-45% Mineral Filled Glossary: Materials: Polymers: Acrylonitrile-Butadiene-Styrene: Flame-Retardant Grades, Molding and Extrusion Glossary: Materials: Polymers: Polyester: Wholly Aromatic (liquid Crystal): 30 - 50% Mineral Filled Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A284 Grade C Related Pages
eFunda: Polymer (Plastic) Supplier Contact Information
Polyester (thermoplastic), poly(ethylene-terephthalate), recycled content, 35% glass/mineral reinforced. Ticona. 90 Morris Ave. Summit, NJ 07901 ...
eFunda Polymers: Properties of Polyester (thermoplastic) {poly ...
eFunda Polymers: Properties of Polyester (thermoplastic) {poly(butylene-
eFunda Polymers: Properties of Polycarbonate {polycarbonate ...
eFunda Polymers: Properties of Polycarbonate {polycarbonate / polyester blends, ... Additives: polycarbonate / polyester blends, impact modified ...
eFunda Polymers: Properties of Polyester (thermoplastic) {poly ...
eFunda Polymers: Properties of Polyester (thermoplastic) {poly(ethylene-
eFunda: Overview of Polymers (Plastics)
Introduction to polymers, their molecular structures and major grouping methods.
eFunda Polymers: Properties of Polyimide {thermoplastic, 30% glass ...
eFunda Polymers: Properties of Polyimide {thermoplastic, 30% glass fiber reinforced} ... State: thermoplastic. Additives: 30% glass fiber reinforced ...
eFunda: Polymer (Plastic) Supplier Contact Information
Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219. Phone: 718-851-8111 ... Bamberger Polymers, Inc. 2 Jericho Plaza. Jericho, NY 11753 ...
eFunda Polymers: Properties of Polyurethane {thermoplastic, 30 ...
... Properties of Polyurethane {thermoplastic, 30% long glass fiber reinforced} ... State: thermoplastic. Additives: 30% long glass fiber reinforced ...
eFunda Polymers: Properties of Thermoplastic elastomers {polyester}
eFunda Polymers: Properties of Thermoplastic elastomers {polyester}
eFunda Polymers: Properties of Polycarbonate {20 - 30% long glass ...
eFunda Polymers: Properties of Polycarbonate {20 - 30% long glass fiber reinforced} ... Additives: 20 - 30% long glass fiber reinforced ...
|
||||||||