Polyethersulfone: Reinforced
Home |
Directory |
Career |
News |
Industrial
|
|
|
|
Glossary » Materials » Polymers » Polyethersulfone » Reinforced
Reinforced PES is a subcategory of Polyethersulfone. The additative is added during the manufacturing process.
Polyethersulfone, also known as PES, is a thermoplastic polycondensate. It is rigid with high strength, transparent, and it retains its properties between 100°C and 150 °C. It has very high dimensional stability with reproducible properties and controllable size of pores. PES is commonly used as membrane filters in applications such as hemodialysis, waste water recovery, food and beverage processing, and gas separation. Polysulfone has the highest service temperature of all melt-processable thermoplastics.
Additional Information
Other common Polyethersulfone (PES) include 10% Glass Fiber Reinforced PES, 20-30% Glass Fiber Reinforced PES, 20% Mineral Filled PES, and 30% Carbon Filled PES.
Related Glossary Pages
Glossary: Materials: Polymers: Polyester: Poly(ethylene-Terephthalate): Recycled Content, 45% Glass Fiber
Glossary: Materials: Alloys: Steel: Tool Steel: AISI S5 Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 8660H Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1019 Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4320H Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 8625 Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A514 Type K Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1117 Glossary: Materials: Polymers: Polyamide: Nylon (PA 66): 15% Glass Fiber Reinforced Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4023 Related Pages
eFunda Polymers: Listing of Polyethersulfone
eFunda Polymers: Listing of Polyethersulfone. ... Specific Grades of Polyethersulfone ... Polyethersulfone, 20-30% glass fiber reinforced. ...
eFunda: Properties of Piezo Material Lead Zirconate Titanate (PZT-5A)
eFunda: Properties of Piezo Material Lead Zirconate Titanate (PZT-5A)
eFunda Polymers: Properties of Polyethersulfone {reinforced}
eFunda Polymers: Properties of Polyethersulfone {reinforced}
eFunda Polymers: Properties of Polyamide {partially aromatic, 50 ...
... Polymers: Properties of Polyamide {partially aromatic, 50% glass fiber reinforced} ... State: partially aromatic. Additives: 50% glass fiber reinforced ...
eFunda Polymers: Properties of Polyethersulfone {30% carbon filled}
eFunda Polymers: Properties of Polyethersulfone {30% carbon filled}
eFunda Polymers: Properties of Polyethersulfone {10% glass fiber ...
eFunda Polymers: Properties of Polyethersulfone {10% glass fiber reinforced}
eFunda Polymers: Properties of Acetal {homopolymer, 20% glass ...
Reinforced Plastics · Maintenance Tech · Modern Plastics · Packaging Digest ... State: homopolymer. Additives: 20% glass reinforced ...
eFunda: Introduction to Porous Media Molding
Polyethylene (PE); Polypropylene (PP); Polystyrene (PS); Polyethersulfone (PES); Nylon (Polyamide, PA); Polytetrafluouroethylene (PTFE) ...
eFunda Polymers: Properties of Polyethersulfone {20-30% glass ...
eFunda Polymers: Properties of Polyethersulfone {20-30% glass fiber reinforced}
eFunda Polymers: Properties of Polyamide {nylon (PA 46), 30% glass ...
eFunda Polymers: Properties of Polyamide {nylon (PA 46), 30% glass reinforced VO
|
||||||||