Alloy With Polystyrene, 30% Glass Fiber Reinforced PPO is a subcategory of Polyphenylene Oxide. The additative is added by weight during the manufacturing process. Its elastic modulus ranges from 1000 to 1300 MPa. Its flexural modulus ranges from 1100 to 1150 MPa. Its tensile strength ranges from 15000 to 18500 MPa at break. Its flexural strength ranges from 20000 to 23000 MPa. Its Izod Impact strength ranges from 1.7 to 2.3 J/cm. Its elongation at break ranges from 2 to 5 %. Its hardness ranges from 115 to 116 Rockwell R. Its specific gravity ranges from 1.27 to 1.36. Its coefficient of thermal expansion ranges from 14 to 25 x 10-6/°C. Its melting temperature ranges from 100 to 125 °C. Its molding pressure ranges from 10 to 40 MPa.
Polyphenylene Oxide, also known as PPO, is a thermoplastic polycondensate. The most common trade name is Ashley. Although it resists many chemicals, it is easily attacked by some hydrocarbons. It has excellent dimensional stability, low moisture absorption, and high mechanical and dielectric strength. PPO is processable by conventional extrusion and injection molding equipment.
Additional Information
Other common Polyphenylene Oxide (PPO) include Alloy With Polystyrene PPO, Alloy With Polystyrene PPO, Alloy With Polystyrene, Impact Modified PPO, Alloy With Polystyrene, 15% Glass Fiber Reinforced PPO, Alloy With Polystyrene, 20% Glass Fiber Reinforced PPO, Alloy With Polystyrene, Mineral Filled PPO, Alloy With Polystyrene, 30% Graphite Fiber EMI Shielding (conductive) PPO, Alloy With Polystyrene, 40% Aluminium Flake EMI Shielding (conductive) PPO, and Alloy With Nylon, Unreinforced PPO.
Related Glossary Pages
Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A302 Grade B
Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 1345 Glossary: Design: Oring: Material: Fluorosilicone Glossary: Materials: Polymers: Liquid Crystal Polymer: PTFE Filled Glossary: Materials: Alloys: Steel: Tool Steel: AISI T1 Glossary: Design: Oring: Material: Hypalon Glossary: Materials: Polymers: Polyacetal: Homopolymer Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 8115 Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1021 Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 9310 Related Pages
eFunda: Listing of Common Polymers (Plastics) in Chronological Order
Polyphenylene Oxide (PPO); 1965. -, Thermoplastic polycondensate. -, It is easily attacked by some hydrocarbons, although it resists many chemicals. ...
eFunda Polymers: Properties of Polyphenylene Oxide (modified ...
Additives: alloy with polystyrene, 30% glass fiber reinforced ... Related Glossary. Materials » Alloys » Steel » Stainless Steel » AISI Type 502 ...
eFunda Polymers: Properties of Polyphenylene Oxide (modified ...
eFunda Polymers: Properties of Polyphenylene Oxide (modified) {alloy with nylon, unreinforced}
eFunda: Polymer (Plastic) Supplier Contact Information
Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219. Phone: 718-851-8111 ... Bamberger Polymers, Inc. 2 Jericho Plaza. Jericho, NY 11753 ...
eFunda Polymers: Properties of ABS {injection molding grade, heat ...
A. Schulman, Akron, OH, 800-662-7203. American Polymers, Inc. Worcester, MA. Ashley Polymers, Brooklyn, NY. BASF Corp. Mount Olive, NJ, 800-BC-RESIN ...
eFunda Polymers: Properties of ABS {injection molding grade, platable}
A. Schulman, Akron, OH, 800-662-7203. American Polymers, Inc. Worcester, MA. Ashley Polymers, Brooklyn, NY. Bamberger Polymers, Inc. Jericho, NY ...
eFunda Polymers: Listing of Polyphenylene Oxide (Ashley)
Polyphenylene Oxide, also known as PPO, has been mass-produced since 1965. ... Polyphenylene Oxide (modified), alloy with polystyrene, 15% glass fiber ...
eFunda Polymers: Properties of ABS {30% glass fiber reinforced ...
eFunda Polymers: Properties of ABS {30% glass fiber reinforced, injection molding grade}
eFunda: Polymers (Plastics) Sorted by Resin Family
Polyphenylene Oxide, (PPO). •, Polyphenylene Sulfide, (PPS). •, Polyphthalamide, (PTA). •, Polysulfone, (PSU). Thermoset: •, Allyl Resin, (Allyl). ...
eFunda: Overview of Polymers (Plastics)
Introduction to polymers, their molecular structures and major grouping methods.
|
||||||||