Polypropylene: Homopolymer: 10 - 40% Calcium Carbonate Filled
Home |
Directory |
Career |
News |
Industrial
|
|
|
|
Glossary » Materials » Polymers » Polypropylene » 10 - 40% Calcium Carbonate Filled
10 - 40% Calcium Carbonate Filled PP is a subcategory of Polypropylene. The additative is added by weight during the manufacturing process. Its elastic modulus ranges from 375 to 500 MPa. Its flexural modulus ranges from 230 to 450 MPa. Its tensile strength ranges from 3400 to 4500 MPa at break. Its flexural strength ranges from 5500 to 7000 MPa. Its compressive strength ranges from 3000 to 7200 MPa. Its Izod Impact strength ranges from 0.5 to 1 J/cm. Its elongation at break ranges from 10 to 245 %. Its hardness ranges from 78 to 99 Rockwell R. Its specific gravity ranges from 0.97 to 1.25. Its coefficient of thermal expansion ranges from 28 to 50 x 10-6/°C. Its molding pressure ranges from 8 to 20 MPa.
Polypropylene, also known as PP, is a thermoplastic, (crystalline), polymer. Common trade names are Marlex HGL and Fortilene 1800 series (FDA materials). homopolymer Its key attributes are high lubricity, high resistance to flexing (excellent material for living hinges), excellent dielectric strength and chemical resistance, good impact strength, and high solvent resistance. It is inexpensive and electroplatable, but it is difficult to paint, print on, or bond to. It will be attacked by fuming nitric acid and degraded by UV and ionizing radiation. PP can be used to make medical syringes, beakers, and parts for auto interiors.
Additional Information
Other common Polypropylene (PP) include Unfilled PP, 10 - 40% Talc Filled PP, 10 - 30% Glass Fiber Reinforced PP, 10 - 50% Mica Filled PP, 40% Glass Fiber Reinforced PP, 20 - 30% Long Glass Fiber Reinforced PP, 40% Long Glass Fiber Reinforced PP, 30% Random Glass Mat PP, Impact Modified, 40% Mica Filled PP, 30% PAN Carbon Fiber EMI Shielding (conductive) PP, Unfilled PP, Unfilled, Impact Modified PP, 10 - 20% Glass Fiber Reinforced PP, and 10 - 40% Talc Filled PP.
Related Glossary Pages
Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C12000
Glossary: Materials: Polymers: Polyphenylene Sulfide: Unfilled Glossary: Materials: Alloys: Titanium Alloy: Wrought: Ti-10V-2Fe-3Al Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 316N Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 5130 Glossary: Materials: Polymers: Polyethylenechlorinates: 30-42% CI: Extrusion and Molding Grades Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 94B17H Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 5160H Glossary: Materials: Alloys: Steel: Carbon Steel: ASTM A570 Grade 30 Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 5130H Related Pages
eFunda Polymers: Properties of Polypropylene {homopolymer, impact ...
eFunda Polymers: Properties of Polypropylene {homopolymer, impact modified, 40% mica filled}
eFunda Polymers: Listing of Liquid Crystal Polymer (Vectra, Xydar)
Liquid Crystal Polymer, also known as LCP, has been mass-produced since 1980. ... Liquid Crystal Polymer, glass fiber reinforced, used for SMT. ...
eFunda Polymers: Properties of Polypropylene {copolymer, 10 - 20 ...
eFunda Polymers: Properties of Polypropylene {copolymer, 10 - 20% glass fiber reinforced}
eFunda: Polymer (Plastic) Supplier Contact Information
Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219. Phone: 718-851-8111
eFunda Polymers: Properties of Polypropylene {homopolymer, 40 ...
eFunda Polymers: Properties of Polypropylene {homopolymer, 40% glass fiber reinforced}
eFunda: Comparisons between Polymers (Plastics) and Metals and ...
CRYSTALLINE POLYMERS: e.g., PPS, PBT (Valox), Polypropylene (PP), have. -, a sharply-defined melting point,. -, high shrinkage after molding, ...
eFunda: Polymers (Plastics) Sorted by Thermoplastic/Thermoset
Polyphenylene Sulfide, (PPS). •, Polyphthalamide, (PTA). •, Polypropylene, (PP). •, Polystyrene, (PS). •, Polysulfone, (PSU). •, Polyurethane, (PU). ...
eFunda: Glossary of Polymers (Plastics)
Common terms used in material science of polymers.
eFunda Polymers: Properties of Polypropylene {homopolymer, 10 - 40 ...
eFunda Polymers: Properties of Polypropylene {homopolymer, 10 - 40% calcium carbonate filled}
eFunda: Polymer (Plastic) Supplier Contact Information
American Polymers, Inc. 53 Millbrook St. P.O. Box 60398. Worcester, MA 01606 ... Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219 ...
|
||||||||