Polyurethane: Thermoplastic: 30% Long Glass Fiber Reinforced
Home |
Directory |
Career |
News |
Industrial
|
|
|
|
Glossary » Materials » Polymers » Polyurethane » 30% Long Glass Fiber Reinforced
30% Long Glass Fiber Reinforced PU is a subcategory of Polyurethane. The additative is added by weight during the manufacturing process. Its compressive strength ranges from 24600 to 25700 MPa. Its Izod Impact strength ranges from 6.2 to 7.5 J/cm. Its molding pressure ranges from 10 to 20 MPa.
Polyurethane, also known as PU, is a thermoplastic or thermoset, (typically reinforced), polyadduct. Common trade names are Estane and Pellanthane. thermoplastic It has high impact resistance, dielectric strength, chemical resistance, and abrasion resistance. It can be made into films, solid moldings, or flexible foams. However, it becomes brittle with prolonged outdoor exposure. It is often used in automotive structural members, computer housings, furniture, and packaging foams.
Additional Information
Other common Polyurethane (PU) include Casting Resin, Liquid PU, Casting Resin, Unsaturated PU, Unreinforced Molding PU, Long Glass Reinforced Molding Compound PU, and 30% PAN Carbon Fiber EMI Shielding (conductive) PU.
Related Glossary Pages
Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C51100
Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A514 Type K Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4037 Glossary: Materials: Alloys: Steel: Stainless Steel: 18-2FM Glossary: Materials: Polymers: Acrylonitrile-Butadiene-Styrene: ABS / PVC: Flame-Retardant Grades, Molding and Extrusion Glossary: Materials: Alloys: Steel: Tool Steel: AISI O1 Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 302 Glossary: Materials: Alloys: Steel: Alloy Steel: ASTM A387 Grade 5 Glossary: Materials: Polymers: Fluoroplastics: Fluorinated Ethylene Propylene: 20% Milled Glass Fiber Glossary: Materials: Alloys: Magnesium Alloy: ASTM QH21A-T6 Related Pages
eFunda Polymers: Properties of Polyurethane {thermoset, casting ...
eFunda Polymers: Properties of Polyurethane {thermoset, casting resin, unsaturated}
eFunda Polymers: Properties of Thermoplastic elastomers {silicone ...
eFunda Polymers: Properties of Thermoplastic elastomers {silicone / polyurethane
eFunda: Polymers (Plastics) Sorted by Resin Family
Thermoplastic: •, Polyurethane, (PU). Thermoset: •, Epoxy. •, Polyurethane, (PU)
eFunda Polymers: Properties of Polyurethane {thermoplastic, 30 ...
eFunda Polymers: Properties of Polyurethane {thermoplastic, 30% PAN carbon fiber
eFunda Polymers: Properties of Polyurethane {thermoset, casting ...
eFunda Polymers: Properties of Polyurethane {thermoset, casting resin, liquid}
eFunda Polymers: Properties of Polyurethane {thermoplastic ...
eFunda Polymers: Properties of Polyurethane {thermoplastic, unreinforced, molding}
eFunda: Chemicals Compatibile with O-Ring Material Polyurethane, Cast
Chemicals Compatible with Polyurethane, Cast (select a chemical to show its compatible O-ring materials). Acetaldehyde (0), Acetamide (0), Acetic Acid, ...
eFunda: Polymer (Plastic) Supplier Contact Information
American Polymers, Inc. 53 Millbrook St. P.O. Box 60398. Worcester, MA 01606 ... Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219 ...
eFunda: Polymer (Plastic) Supplier Contact Information
Ashley Polymers. 5114 Ft. Hamilton Pkwy. Brooklyn, NY 11219. Phone: 718-851-8111
eFunda: Glossary of Polymers (Plastics)
Common terms used in material science of polymers.
|
||||||||