Unplasticized Barrier Film Resins PVDC is a subcategory of Polyvinylidene Chloride. The additative is added during the manufacturing process. Its elastic modulus ranges from 50 to 80 MPa. Its Izod Impact strength ranges from 0.3 to 1 J/cm. Its elongation at break ranges from 350 to 400 %. Its hardness ranges from 98 to 106 Rockwell R. Its specific gravity ranges from 1.65 to 1.7. Its molding pressure ranges from 3 to 30 MPa.
Polyvinylidene Chloride, also known as PVDC, is a thermoplastic polymer. Common trade names include Diofan, Ixan, and Saran. copolymer It has high hardness and good abrasion resistance. It is typically used as one of the components in a copolymer.
Additional Information
Other common Polyvinylidene Chloride (PVDC) include Injection Molding PVDC, and Plasticized Barrier Film Resins PVDC.
Related Glossary Pages
Glossary: Materials: Polymers: Polycarbonate: 20 - 30% Long Glass Fiber Reinforced: Flame-Retardant Grade
Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C33500 Glossary: Materials: Alloys: Copper Alloy: Wrought: UNS C41100 Glossary: Materials: Alloys: Steel: Stainless Steel: AISI Type 305 Glossary: Materials: Polymers: Polystyrene: Styrene / Methyl-Methacrylate Copolymer Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 5130 Glossary: Materials: Alloys: Copper Alloy: Wire: AWG-8 Glossary: Materials: Alloys: Steel: Alloy Steel: SAE 965X Glossary: Materials: Alloys: Steel: Alloy Steel: AISI 4820 Glossary: Materials: Alloys: Steel: Carbon Steel: AISI 1045 Related Pages
eFunda Polymers: Properties of Polyvinylidene Chloride {copolymer ...
eFunda Polymers: Properties of Polyvinylidene Chloride {copolymer, injection molding}
eFunda: Listing of Common Polymers (Plastics) in Chronological Order
Polyvinylidene Chloride (PVDC); 1930's. -, Thermoplastic polymer. -, Typically used as one of the components in a copolymer. ...
eFunda Polymers: Listing of Polyvinylidene Chloride (Diofan, Ixan ...
Polyvinylidene Chloride, also known as PVDC, has been mass-produced since 1930's ... Polyvinylidene Chloride, copolymer, unplasticized, barrier film resins. ...
eFunda: Polymer (Plastic) Supplier Contact Information
Polyvinylidene Chloride, copolymer, injection molding. Dow Plastics. 690 Bldg. Midland, MI 48640. Toll Free: 800-441-4369. Phone: 517-832-1466 ...
eFunda: Polymer (Plastic) Supplier Contact Information
Polyvinylidene Chloride, copolymer, unplasticized, barrier film resins. Dow Plastics. 690 Bldg. Midland, MI 48640. Toll Free: 800-441-4369 ...
eFunda: Polymers (Plastics) Sorted by Thermoplastic/Thermoset
Polysulfone, (PSU). •, Polyurethane, (PU). •, Polyvinylchloride, (PVC). •, Polyvinylidene Chloride, (PVDC). •, Thermoplastic elastomers, (TPE). ...
eFunda: Polymers (Plastics) Sorted by Resin Family
Polymethylpentene, (PMP). •, Polypropylene, (PP). •, Polystyrene, (PS). •, Polyvinylchloride, (PVC). •, Polyvinylidene Chloride, (PVDC). ...
eFunda Polymers: Properties of Polyvinylidene Chloride {copolymer ...
eFunda Polymers: Properties of Polyvinylidene Chloride {copolymer, unplasticized
eFunda: Listing of Common Polymers (Plastics)
Polyvinylchloride, (PVC), Thermoplastic polymer. Polyvinylidene Chloride, (PVDC)
|
|||||||||||||||||||||||||