Steel
Designation Class Alloy Type AISI
ASTM A505  Alloy steel  Nickel-chromium-molybdenum steel  8740 
ASTM A505  Alloy steel  Silicon-manganese steel  9260 
ASTM A505  Alloy steel  Nickel-chromium-molybdenum steel  E4340 