AA 1350 |
 |
|
| Category | Aluminum Alloy |
| Class | Wrought |
| Composition |
 |
|
| Element | Weight % |
| Al |
99.50 (min) |
|
|
| Mechanical Properties |
 |
|
| Properties | Conditions |
| T (°C) | Treatment |
| Density (×1000 kg/m3) |
2.6-2.8
|
25 |
|
| Poisson's Ratio |
0.33 |
25 |
|
| Elastic Modulus (GPa) |
70-80
|
25 |
|
| Tensile Strength (Mpa) |
97 |
25 |
H12 more |
| Yield Strength (Mpa) |
83 |
| Elongation (%) |
|
| Reduction in Area (%) |
|
| Shear Strength (MPa) |
62 |
25 |
H12 more |
| Fatigue Strength (MPa) |
48 |
25 |
H19 |
| Thermal Properties |
 |
|
| Properties | Conditions |
| T (°C) | Treatment |
| Thermal Conductivity (W/m-K) |
230 |
25 |
All Hlx more |
| Electric Properties |
 |
|
| Properties | Conditions |
| T (°C) | Treatment |
| Electric Resistivity (10-9W-m) |
28 |
25 |
Hlx more |
|