| Designations |
France: AFNOR Z 6 CND 17.11
Germany: DIN 1.4401
Italy: UNI X 5 CrNIMo 17 12
Japan: JIS SUH 309
, JIS SUS 316
, JIS SUS Y 316
Sweden: SS 2347
United Kingdom: B.S. 316 S 16
, B.S. 316 S 18
, B.S. 316 S 25
, B.S. 316 S 26
, B.S. 316 S 30
, B.S. 316 S 40
, B.S. 316 S 41
, B.S. En. 58 H
United States: AMS 5524
, AMS 5573
, AMS 5648
, AMS 5690
, AMS 5691
, ASME SA182
, ASME SA193
, ASME SA194
, ASME SA213
, ASME SA240
, ASME SA249
, ASME SA312
, ASME SA320
, ASME SA358
, ASME SA376
, ASME SA403
, ASME SA409
, ASME SA430
, ASME SA479
, ASME SA688
, ASTM A167
, ASTM A182
, ASTM A193
, ASTM A194
, ASTM A213
, ASTM A240
, ASTM A249
, ASTM A269
, ASTM A276
, ASTM A312
, ASTM A313
, ASTM A314
, ASTM A320
, ASTM A358
, ASTM A368
, ASTM A376
, ASTM A403
, ASTM A409
, ASTM A430
, ASTM A473
, ASTM A478
, ASTM A479
, ASTM A580
, FED QQ-S-763
, FED QQ-S-766
, FED QQ-W-423
, MIL SPEC MIL-S-5059
, MIL SPEC MIL-S-862
, SAE 30316
, SAE J405 (30316)
, UNS S31600
|