Materials: Metal Alloys: Properties
engineering fundamentals Alloys Properties
Directory | Career | News | Standards | Industrial | SpecSearch®
 
 
Metal Alloys
Alloy Home
Ferrous Alloys
Steels in General
Alloy Steels
Carbon Steels
Stainless Steels
Tool Steels
Non-Ferrous Alloys
Aluminum Alloys
Copper Alloys
Magnesium Alloys
Titanium Alloys
Specific Alloy
General Information
Further Details
Resources
Bibliography


Login

Home Membership Store Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
Ti-11.5Mo-6Zr-4.5Sn
Category Titanium Alloy
Class Wrought
Type Beta alloy
Designations United States: MIL-T-9047, AMS 4977, AMS 4980

Composition
ElementWeight %
Mo  11.5 
Zr  6 
Sn  4.5 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 4.51 25  
Poisson's Ratio 0.33 25  
Elastic Modulus (GPa) 103.4 25  
Tensile Strength (Mpa) 1386  25  solution+age  
Yield Strength (Mpa) 1317 
Elongation (%) 11 
Reduction in Area (%)  