Materials: Metal Alloys: Properties
engineering fundamentals Alloys Properties
Directory | Career | News | Standards | Industrial | SpecSearch®
 
 
Metal Alloys
Alloy Home
Ferrous Alloys
Steels in General
Alloy Steels
Carbon Steels
Stainless Steels
Tool Steels
Non-Ferrous Alloys
Aluminum Alloys
Copper Alloys
Magnesium Alloys
Titanium Alloys
Specific Alloy
General Information
Further Details
Resources
Bibliography


Login

Home Membership Store Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
99.1 Ti
Category Titanium Alloy
Class Wrought
Type Commercially Pure
Designations United States: ASTM B265 Grade3, ASTM B348 Grade3, ASTM B381 Grade3, MIL-T-9046, ,AMS 4900

Composition
ElementWeight %
Ti  99.1 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 4.51 25  
Poisson's Ratio 0.34 25  
Elastic Modulus (GPa) 103.4 25  
Tensile Strength (Mpa) 234  315 more annealed  
Yield Strength (Mpa) 138 
Elongation (%) 34 
Reduction in Area (%) 75 
Hardness (HB) 225  25  annealed 
Impact Strength (J)
(Charpy)
38  25  annealed  

Thermal Properties
Properties Conditions 
T (°C)Treatment
Thermal Expansion (10-6/ºC) 8.6  20-100 more  