eFunda: Properties of Alloy Steel Alloy Steel Alloy Steel AA 3004
Alloy Steel Alloy Steel Alloy Steel AA 3004
Directory
|
Career
|
News
|
Standards
|
Industrial
|
SpecSearch®
Keywords
AISI (US)
UNS (US)
SAE (US)
ASTM (US)
AMS (US)
ASME (US)
MIL (US)
FED (US)
DIN (DEU)
JIS (JPN)
AFNOR(FR)
B.S. (UK)
SS (SWE)
UNI (ITA)
Aluminum
Metal Alloys
Alloy Home
Steels
Alloy Steels
General Information
Properties
Classification
Standard
H-Steels
HSLA
Alloy Steel List
AISI 1xxx
AISI 2xxx
AISI 3xxx
AISI 4xxx
AISI 5xxx
AISI 6xxx
AISI 8xxx
AISI 9xxx
*
For other AISI or Non-AISI, please use the search function above or check Grades.
ASTM Steels
Resources
Bibliography
Trade Publications
Photonics Spectra
appliance DESIGN
Paint & Coatings
NASA Tech Briefs
Maintenance Tech
Industrial Heating
more
Login
Home
Membership
Store
Forum
Search Member
Calculators
Materials
Design
Processes
Units
Formulas
Math
AA 3004
Conditions
Fatigue Strength
(MPa)
T
(°C)
Treatment
25
H32
105
25
H34
105
25
H36
110
25
H38
110
25
O
97
Glossary
Materials » Alloys » Steel » Alloy Steel » AISI 8622
Materials » Alloys » Steel » Tool Steel » AISI T6
Materials » Alloys » Aluminum Alloy » Wrought » AA 1060
Materials » Alloys » Steel » Alloy Steel » AISI 8660H
Materials » Alloys » Aluminum Alloy » Wrought » AA 5652
Materials » Alloys » Steel » Alloy Steel » AISI 4340
Materials » Alloys » Steel » Alloy Steel » AISI 51B60H
Materials » Alloys » Steel » Tool Steel » AISI T5
Materials » Alloys » Steel » Alloy Steel » ASTM A542
Materials » Alloys » Steel » Alloy Steel » AISI 51B60H
Home
Membership
About Us
Privacy
Disclaimer
Contact
Advertise
Copyright © 2009 eFunda, Inc.