eFunda: Properties of Alloy Steel AA 5052
engineering fundamentals Alloy Steel AA 5052
Directory | Career | News | Standards | Industrial | SpecSearch®
 
 
Metal Alloys
Alloy Home
Steels
Alloy Steels
General Information
Properties
Classification
Standard
H-Steels
HSLA
Alloy Steel List
AISI 1xxx
AISI 2xxx
AISI 3xxx
AISI 4xxx
AISI 5xxx
AISI 6xxx
AISI 8xxx
AISI 9xxx
* For other AISI or Non-AISI, please use the search function above or check Grades.
ASTM Steels
Specific Alloy Steel
General Information
Resources
Bibliography


Login

Home Membership Store Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
AA 5052
Category Aluminum Alloy
Class Wrought

Composition
ElementWeight %
Al  97.2 
Mg  2.5 
Cr  0.25 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 2.68 25  
Poisson's Ratio 0.33 25  
Elastic Modulus (GPa) 70-80 25  
Tensile Strength (Mpa) 230  25  H32  more
Yield Strength (Mpa) 195 
Elongation (%) 12 
Reduction in Area (%)  
Hardness (HB500) 60  25  H32 more
Shear Strength (MPa) 140  25  H32  more
Fatigue Strength (MPa) 115  25  H32  more

Thermal Properties
Properties Conditions 
T (°C)Treatment
Thermal Expansion (10-6/ºC) 23.8  20-100  
Thermal Conductivity (W/m-K) 137  25  H38 more

Electric Properties
Properties Conditions 
T (°C)Treatment
Electric Resistivity (10-9W-m) 49  25  H38 more