eFunda: Properties of Alloy Steel Alloy Steel Alloy Steel Alloy Steel Alloy Steel Alloy Steel AA 6009
engineering fundamentals Alloy Steel Alloy Steel Alloy Steel Alloy Steel Alloy Steel Alloy Steel AA 6009
Directory | Career | News | Standards | Industrial | SpecSearch®
 
 
Metal Alloys
Alloy Home
Steels
Alloy Steels
General Information
Properties
Classification
Standard
H-Steels
HSLA
Alloy Steel List
AISI 1xxx
AISI 2xxx
AISI 3xxx
AISI 4xxx
AISI 5xxx
AISI 6xxx
AISI 8xxx
AISI 9xxx
* For other AISI or Non-AISI, please use the search function above or check Grades.
ASTM Steels
Specific Alloy Steel
General Information
Further Details
Resources
Bibliography


Login

Home Membership Store Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
AA 6009
Category Aluminum Alloy
Class Wrought

Composition
ElementWeight %
Al  97.7 
Si  0.80 
Cu  0.35 
Mn  0.5 
Mg  0.60 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 2.6-2.8 25  
Poisson's Ratio 0.33 25  
Elastic Modulus (GPa) 70-80 25  
Tensile Strength (Mpa) 235  25  T4  more
Yield Strength (Mpa) 130 
Elongation (%) 24 
Reduction in Area (%)  
Hardness (HR15T) 70  25  T4 
Shear Strength (MPa) 150  25  T4  
Fatigue Strength (MPa) 115  25  T4  

Thermal Properties
Properties Conditions 
T (°C)Treatment
Thermal Conductivity (W/m-K) 205  25  more

Electric Properties
Properties Conditions 
T (°C)Treatment
Electric Resistivity (10-9W-m) 32  25  more