eFunda: Properties of Alloy Steel AISI 4135
engineering fundamentals Alloy Steel AISI 4135
Directory | Career | News | Standards | Industrial | SpecSearch®
Metal Alloys
Alloy Home
Steels
Alloy Steels
General Information
Properties
Classification
Standard
H-Steels
HSLA
Alloy Steel List
AISI 1xxx
AISI 2xxx
AISI 3xxx
AISI 4xxx
AISI 5xxx
AISI 6xxx
AISI 8xxx
AISI 9xxx
* For other AISI or Non-AISI, please use the search function above or check Grades.
ASTM Steels
Resources
Bibliography
Login

Home Membership Magazines Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
AISI 4135
Category Steel
Class Alloy steel
Type Standard
Common Names Chromium-molybdenum steel
Designations  France: AFNOR 35 CD 4 , AFNOR 35 CD 4 TS
Germany: DIN 1.7220
Italy: UNI 34 CrMo 4 KB , UNI 35 CrMo 4 , UNI 35 CrMo 4 F
Japan: JIS SCCrM 3 , JIS SCM 1
Sweden: SS 2234
United Kingdom: B.S. 708 A 37
United States: AMS 6365C , AMS 6365E , AMS 6372C , AMS 6372D , ASTM A355 , ASTM A519 , ASTM A711 , MIL SPEC MIL-S-16974 , MIL SPEC MIL-S-18733 , SAE J404 , SAE J412 , SAE J770 , UNS G41350

Composition

ElementWeight %
C  0.33-0.38 
Mn  0.70-0.90 
P  0.035 (max) 
S  0.04 (max) 
Si  0.15-0.30 
Cr  0.30-1.10 
Mo  0.15-0.25 

Mechanical Properties

Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 7.7-8.03 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 190-210 25  