ASTM A387 Grade 9 |
 |
|
| Category | Steel |
| Class | Alloy steel |
| Designations | United States: UNS S50400 |
| Composition |
 |
|
| Element | Weight % |
| C |
0.15 |
| Mn |
0.30-0.60 |
| P |
0.03 |
| S |
0.030 |
| Si |
1.00 |
| Cr |
8.00-10.00 |
| Mo |
0.90-1.10 |
|
|
| Mechanical Properties |
 |
|
| Properties | Conditions |
| T (°C) | Treatment |
| Density (×1000 kg/m3) |
7.7-8.03
|
25 |
|
| Poisson's Ratio |
0.27-0.30 |
25 |
|
| Elastic Modulus (GPa) |
190-210
|
25 |
|
|