ASTM A514 Type D |
 |
|
| Category | Steel |
| Class | Alloy steel |
| Designations | United States: UNS K11662 |
| Composition |
 |
|
| Element | Weight % |
| C |
0.13-0.20 |
| Mn |
0.40-0.70 |
| P |
0.035 |
| S |
0.04 |
| Si |
0.20-0.35 |
| Cr |
0.85-1.20 |
| Mo |
0.15-0.25 |
| Ti |
0.04-0.10 |
| Cu |
0.20-0.40 |
| B |
0.0015-0.005 |
|
|
| Mechanical Properties |
 |
|
| Properties | Conditions |
| T (°C) | Treatment |
| Density (×1000 kg/m3) |
7.7-8.03
|
25 |
|
| Poisson's Ratio |
0.27-0.30 |
25 |
|
| Elastic Modulus (GPa) |
190-210
|
25 |
|
|