ASTM A588 Grade H |
 |
|
| Category | Steel |
| Class | Alloy steel |
| Designations | United States: UNS K12032 |
| Composition |
 |
|
| Element | Weight % |
| C |
0.20 (max) |
| Mn |
1.25 (max) |
| P |
0.035 |
| S |
0.04 |
| Si |
0.25-0.75 |
| Cr |
0.10-0.25 |
| Ni |
0.30-0.60 |
| Mo |
0.15 (max) |
| V |
0.02-0.10 |
| Cu |
0.20-0.35 |
| Ti |
0.005-0.030 |
|
|
| Mechanical Properties |
 |
|
| Properties | Conditions |
| T (°C) | Treatment |
| Density (×1000 kg/m3) |
7.7-8.03
|
25 |
|
| Poisson's Ratio |
0.27-0.30 |
25 |
|
| Elastic Modulus (GPa) |
190-210
|
25 |
|
|