eFunda: Properties of Aluminum Alloy Aluminum Alloy Aluminum Alloy Aluminum Alloy 319.0
engineering fundamentals Aluminum Alloy Aluminum Alloy Aluminum Alloy Aluminum Alloy 319.0
Directory | Career | News | Standards | Industrial | SpecSearch®
 
 
Metal Alloys
Alloy Home
Aluminum Alloys
General Information
Properties
Temper
Al Alloy Types
Cast Alloys
Wrought Alloys
Al Alloy List
Wrought:
   AA 1xxx
   AA 2xxx
   AA 3xxx
   AA 4xxx
   AA 5xxx
   AA 6xxx
   AA 7xxx
Cast:
   2xx.0 or x2xx.0
   3xx.0 or x3xx.0
   4xx.0 or x4xx.0
   5xx.0 or x5xx.0
   7xx.0
   8xx.0
Specific Al Alloy
General Information
Further Details
Resources
Bibliography


Login

Home Membership Store Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
319.0
Category Aluminum Alloy
Class Cast

Composition
ElementWeight %
Al  90.50 
Cu  3.50 
Si  6.00 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 2.79 25  
Poisson's Ratio 0.33 25  
Elastic Modulus (GPa) 70-80 25  
Tensile Strength (Mpa) 235  25  F (permanent mold casting) more
Yield Strength (Mpa) 130 
Elongation (%) 2.5 
Reduction in Area (%)  

Thermal Properties
Properties Conditions 
T (°C)Treatment
Thermal Expansion (10-6/ºC) 21.5  20-100  