| Designations |
France: AFNOR CC 20 Germany: DIN 1.0402 Italy: UNI C 20 Sweden: SS 1450 United Kingdom: B.S. 040 A 20 , B.S. 070 M 20 United States: AMS 5032 , AMS 5032B , AMS 5045 , AMS 5045C , ASTM A108 , ASTM A29 , ASTM A510 , ASTM A519 , ASTM A544 , ASTM A575 , ASTM A576 , ASTM A659 , MIL SPEC MIL-S-11310 (CS1020) , SAE J403 , SAE J412 , SAE J414 , UNS G10200
|