AISI 1524 |
 |
|
| Category | Steel |
| Class | Carbon steel |
| Type | Standard |
| Designations | United States: UNS G15240 |
| Composition |
 |
|
| Element | Weight % |
| C |
0.19-0.25 |
| Mn |
1.35-1.65 |
| P |
0.04 (max) |
| S |
0.05 (max) |
|
|
| Mechanical Properties |
 |
|
| Properties | Conditions |
| T (°C) | Treatment |
| Density (×1000 kg/m3) |
7.7-8.03
|
25 |
|
| Poisson's Ratio |
0.27-0.30 |
25 |
|
| Elastic Modulus (GPa) |
190-210
|
25 |
|
| Thermal Properties |
 |
|
| Properties | Conditions |
| T (°C) | Treatment |
| Thermal Expansion (10-6/ºC) |
11.9 |
20-100 more |
|
| Thermal Conductivity (W/m-K) |
46 |
0 more |
|
| Specific Heat (J/kg-K) |
477 |
50-100 more |
|
| Electric Properties |
 |
|
| Properties | Conditions |
| T (°C) | Treatment |
| Electric Resistivity (10-9W-m) |
208 |
20 more |
|
|